Materials / Compare

Aluminum 5052-H32 vs. Iron

Compare Aluminum 5052-H32 vs. Iron strength, stiffness, weight and thermal properties.

Aluminum 5052-H32Wrought
IronWrought
MechanicalAluminum 5052-H32Iron
Yield strength195MPa1186MPa2
Ultimate tensile strength230MPa1290MPa226% stronger
Elongation at break12%138%23.17x more ductile
Young's modulus (stiffness)70GPa1207GPa22.96x stiffer
Density2,685kg/m³32.93x lighter7,860kg/m³2
Strength to weight72.6kN·m/kg3.07x higher23.7kN·m/kg
Stiffness to weight26.1MN·m/kg26.3MN·m/kg1% higher
Poisson's ratio0.3330.2824
Shear modulus26.3GPa80.7GPa3.07x stiffer in shear
Bulk modulus68.6GPa158GPa2.31x higher
Speed of sound5,106m/s5,132m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Iron
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Iron
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 5052-H32Iron
Thermal conductivitybase material138W/m·K11.89x more heat through a fin73.2W/m·K2
Thermal expansion23.8µm/m·K1mean13.7µm/m·K21.74x less
100 mm part over a 50 °C swing119µm growth68.5µm growth1.74x less
Specific heatat 100 °C963J/kg·K32.14x higher450J/kg·K2
Heats up and cools (diffusivity)53.4mm²/s2.58x faster20.7mm²/s
Thermal shock resistance10,822W/m3.14x more resistant3,447W/m
Melting pointmelting range605–650°C11,532°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Iron
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 5052-H32Iron
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, Cleveland-Cliffs, U.S. Department of Defense, National Institute of Standards and Technology
Aluminum 5052-H32
5052-H32, Kaiser Aluminum tube & pipe typical datasheet (mechanical, CTE, melting); MIL-HDBK-5J (Poisson, density, specific heat)
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
  1. 1
    Alloy 5052 Tube & Pipe Technical DataKaiser Aluminumarchived copyAluminum 5052-H32 · Yield strength: typical, 0.2% offsetAluminum 5052-H32 · Ultimate tensile strength: typicalAluminum 5052-H32 · Elongation at break: typicalAluminum 5052-H32 · Young's modulus (stiffness): typicalAluminum 5052-H32 · Thermal conductivity: base material: 5052 in O temper (same alloy, annealed); Kaiser typicalAluminum 5052-H32 · Thermal expansion: typical, mean 20-100 °CAluminum 5052-H32 · Melting point: melting range
  2. 2
    ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 5052-H32 · Density: nominalAluminum 5052-H32 · Poisson's ratio: typical (handbook physical constant)Aluminum 5052-H32 · Specific heat: at 100 °C (212 °F); table covers O, H32, H34, H36, H38
  4. 4
    Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 5052-H32 stronger than Iron?

Aluminum 5052-H32 is stronger: its yield strength is 195 MPa against 186 MPa for Iron (5%).

Which is lighter, Aluminum 5052-H32 or Iron?

Aluminum 5052-H32 is lighter: 2,685 kg/m³ against 7,860 kg/m³ for Iron.

Which is stiffer, Aluminum 5052-H32 or Iron?

Iron is stiffer: Young's modulus 207 GPa against 70 GPa for Aluminum 5052-H32, so the same part in Iron deflects less under the same load.

Which is lighter for the same job, Aluminum 5052-H32 or Iron?

For the same stiffness or strength: Aluminum 5052-H32 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate; Iron is lighter for a stiff rod or tie (tension).

Part that must beAluminum 5052-H32Iron
Stiff rod or tie (tension)1% heavierlighter
Stiff beam (bending)lighter1.7x heavier
Stiff panel or platelighter2.04x heavier
Strong rod or tielighter3.07x heavier
Strong beamlighter3.02x heavier
Strong panel or platelighter3x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 5052-H32 or Iron?

Iron stretches further before it breaks: 38% elongation at break against 12% for Aluminum 5052-H32.

Thermal

Which conducts heat better, Aluminum 5052-H32 or Iron?

Aluminum 5052-H32 conducts heat better: 138 W/m·K against 73.2 W/m·K for Iron.

Which expands less with temperature?

Iron expands less: 13.7 µm/m·K against 23.8 µm/m·K for Aluminum 5052-H32.