Materials / Compare

Aluminum 7075-T6 vs. Ceramic Aluminum Nitride

Compare Aluminum 7075-T6 vs. Ceramic Aluminum Nitride strength, stiffness, weight and thermal properties.

Aluminum 7075-T6Wrought
Ceramic Aluminum NitrideSintered ceramic (pressed and fired)
MechanicalAluminum 7075-T6Ceramic Aluminum Nitride
Yield strength503MPa1none (brittle)
Ultimate tensile strength572MPa1not sourced
Flexural strengthnot sourced310MPa2
Elongation at break11%1none (brittle)
Young's modulus (stiffness)71GPa1320GPa24.51x stiffer
Density2,800kg/m³321% lighter3,400kg/m³2
Strength to weight180kN·m/kgnot sourced
Stiffness to weight25.4MN·m/kg94.1MN·m/kg3.71x higher
Poisson's ratio0.3340.242
Shear modulus26.7GPa129GPa4.83x stiffer in shear
Bulk modulus69.6GPa205GPa2.95x higher
Speed of sound5,036m/s9,701m/s1.93x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Ceramic Aluminum Nitride
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 7075-T6Ceramic Aluminum Nitride
Thermal conductivity130W/m·K3150W/m·K215% more heat through a fin
Thermal expansion23.4µm/m·K3mean4.6µm/m·K25.09x less
100 mm part over a 50 °C swing117µm growth23µm growth5.09x less
Specific heat960J/kg·K335% higher710J/kg·K2
Heats up and cools (diffusivity)48.4mm²/s62.1mm²/s28% faster
Thermal shock resistance26,370W/mnot sourced
Melting pointmelting range532–635°C3not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Ceramic Aluminum Nitride
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Ceramic Aluminum Nitride
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, KYOCERA Fineceramics Europe, U.S. Department of Defense
Aluminum 7075-T6
7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J
Ceramic Aluminum Nitride
KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
  1. 1
    Alloy 7075 Rod & Bar Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 7075-T6 · Ultimate tensile strength: typicalAluminum 7075-T6 · Elongation at break: typical, in 4DAluminum 7075-T6 · Young's modulus (stiffness): typical
  2. 2
    AN216A Aluminium Nitride Data Sheet (2023)KYOCERA Fineceramics Europearchived copyCeramic Aluminum Nitride · Flexural strength: 3-point bending strength (JIS R 1601)Ceramic Aluminum Nitride · Young's modulus (stiffness): typical (JIS R 1602)Ceramic Aluminum Nitride · Density: typical (JIS R 1634)Ceramic Aluminum Nitride · Poisson's ratio: typical (JIS R 1602)Ceramic Aluminum Nitride · Thermal conductivity: typical (JIS R 1611)Ceramic Aluminum Nitride · Thermal expansion: mean, 40-400 °C (JIS R 1618)Ceramic Aluminum Nitride · Specific heat: typical (JIS R 1611)
  3. 3
    Alloy 7075 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Density: nominalAluminum 7075-T6 · Thermal conductivity: typical, 20 °C, T651Aluminum 7075-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 7075-T6 · Specific heat: typical, at 100 °CAluminum 7075-T6 · Melting point: melting range
  4. 4
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum 7075-T6 · Poisson's ratio: typical (handbook physical constant)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Which is lighter, Aluminum 7075-T6 or Ceramic Aluminum Nitride?

Aluminum 7075-T6 is lighter: 2,800 kg/m³ against 3,400 kg/m³ for Ceramic Aluminum Nitride.

Which is stiffer, Aluminum 7075-T6 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 71 GPa for Aluminum 7075-T6, so the same part in Ceramic Aluminum Nitride deflects less under the same load.

Which is lighter for the same job, Aluminum 7075-T6 or Ceramic Aluminum Nitride?

For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beAluminum 7075-T6Ceramic Aluminum Nitride
Stiff rod or tie (tension)3.71x heavierlighter
Stiff beam (bending)1.75x heavierlighter
Stiff panel or plate36% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum 7075-T6 or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride conducts heat better: 150 W/m·K against 130 W/m·K for Aluminum 7075-T6.

Which expands less with temperature?

Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 23.4 µm/m·K for Aluminum 7075-T6.