Materials / Compare

Aluminum 7050-T7451 vs. Aluminum 7075-T6

Compare Aluminum 7050-T7451 vs. Aluminum 7075-T6 strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7050-T7451Wrought
Aluminum 7075-T6Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength469MPasourcetypical, longitudinal, 0.2% offset503MPasourcetypical, 0.2% offset, .500 in dia specimen
Ultimate tensile strength524MPasourcetypical, longitudinal572MPasourcetypical
Elongation at break11%sourcetypical, longitudinal11%sourcetypical, in 4D
Young's modulus (stiffness)70.3GPasourcetypical71GPasourcetypical
Density2,830kg/m³sourcenominal2,800kg/m³sourcenominal
Strength to weight166kN·m/kg180kN·m/kg8% higher
Stiffness to weight24.8MN·m/kg25.4MN·m/kg2% higher
Poisson's ratio0.33sourcetypical (handbook physical constant)0.33sourcetypical (handbook physical constant)
Shear modulus26.4GPa26.7GPa
Bulk modulus68.9GPa69.6GPa
Speed of sound4,984m/s5,036m/s
Thermal
Thermal conductivity157W/m·Ksourcetypical, 20 °C130W/m·Ksourcetypical, 20 °C, T651
Thermal expansion23.5µm/m·Ksourcetypical, mean 20-100 °C23.4µm/m·Ksourcetypical, mean 20-100 °C
100 mm part over a 50 °C swing118µm growth117µm growth
Specific heat860J/kg·Ksourcetypical, at 100 °C960J/kg·Ksourcetypical, at 100 °C
Heats up and cools (diffusivity)64.5mm²/s33% faster48.4mm²/s
Thermal shock resistance29,862W/m13% more resistant26,370W/m
Melting point524–635°Csourcemelting range532–635°Csourcemelting range
Values for7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 7050-T7451 stronger than Aluminum 7075-T6?

Aluminum 7075-T6 is stronger: its yield strength is 503 MPa against 469 MPa for Aluminum 7050-T7451 (7%).

Which is lighter, Aluminum 7050-T7451 or Aluminum 7075-T6?

Aluminum 7075-T6 is lighter: 2,800 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.

Which is stiffer, Aluminum 7050-T7451 or Aluminum 7075-T6?

Aluminum 7075-T6 is stiffer: Young's modulus 71 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Aluminum 7075-T6 deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Aluminum 7075-T6?

For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 7050-T7451Aluminum 7075-T6
Stiff rod or tie (tension)2% heavierlighter
Stiff beam (bending)2% heavierlighter
Stiff panel or plate1% heavierlighter
Strong rod or tie8% heavierlighter
Strong beam6% heavierlighter
Strong panel or plate5% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 7050-T7451 or Aluminum 7075-T6?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 130 W/m·K for Aluminum 7075-T6.

Which expands less with temperature?

Aluminum 7075-T6 expands less: 23.4 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 7050-T7451Aluminum 7075-T6
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 7050-T7451Aluminum 7075-T6
Strength against density

Related comparisons