Materials / Compare

Aluminum vs. Aluminum 7050-T7451

Compare Aluminum vs. Aluminum 7050-T7451 strength, stiffness, weight and thermal properties.

Change either side
AluminumWrought
Aluminum 7050-T7451Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength276MPasourcetypical, 0.2% offset, .500 in dia specimen469MPasourcetypical, longitudinal, 0.2% offset
Ultimate tensile strength310MPasourcetypical524MPasourcetypical, longitudinal
Elongation at break17%sourcetypical, in 4D, 0.500 in dia specimen11%sourcetypical, longitudinal
Young's modulus (stiffness)68.3GPasourcetypical70.3GPasourcetypical
Density2,700kg/m³sourcenominal2,830kg/m³sourcenominal
Strength to weight102kN·m/kg166kN·m/kg1.62x higher
Stiffness to weight25.3MN·m/kg2% higher24.8MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant)0.33sourcetypical (handbook physical constant)
Shear modulus25.7GPa26.4GPa3% stiffer in shear
Bulk modulus67GPa68.9GPa
Speed of sound5,030m/s4,984m/s
Thermal
Thermal conductivity167W/m·Ksourcetypical, 20 °C157W/m·Ksourcetypical, 20 °C
Thermal expansion23.6µm/m·Ksourcetypical, mean 20-100 °C23.5µm/m·Ksourcetypical, mean 20-100 °C
100 mm part over a 50 °C swing118µm growth118µm growth
Specific heat896J/kg·Ksourcetypical, at 100 °C860J/kg·Ksourcetypical, at 100 °C
Heats up and cools (diffusivity)69mm²/s7% faster64.5mm²/s
Thermal shock resistance19,159W/m29,862W/m1.56x more resistant
Melting point582–652°Csourcesolidus-liquidus524–635°Csourcemelting range
Values for6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum stronger than Aluminum 7050-T7451?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 276 MPa for Aluminum (1.7x).

Which is lighter, Aluminum or Aluminum 7050-T7451?

Aluminum is lighter: 2,700 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.

Which is stiffer, Aluminum or Aluminum 7050-T7451?

Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 68.3 GPa for Aluminum, so the same part in Aluminum 7050-T7451 deflects less under the same load.

Which is lighter for the same job, Aluminum or Aluminum 7050-T7451?

For the same stiffness or strength: Aluminum is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Aluminum 7050-T7451 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminumAluminum 7050-T7451
Stiff rod or tie (tension)lighter2% heavier
Stiff beam (bending)lighter3% heavier
Stiff panel or platelighter4% heavier
Strong rod or tie1.62x heavierlighter
Strong beam36% heavierlighter
Strong panel or plate24% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum or Aluminum 7050-T7451?

Aluminum conducts heat better: 167 W/m·K against 157 W/m·K for Aluminum 7050-T7451.

Which expands less with temperature?

Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 23.6 µm/m·K for Aluminum.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminumAluminum 7050-T7451
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminumAluminum 7050-T7451