Materials / Aluminum
Aluminum 7050-T7451
Aluminum 7050-T7451 strength, stiffness, density and thermal properties, with their source.
A bracket in Aluminum 7050-T7451, brushed finish.
| Process | Wrought |
|---|---|
| Mechanical | |
| Yield strength | 469MPasourcetypical, longitudinal, 0.2% offset |
| Ultimate tensile strength | 524MPasourcetypical, longitudinal |
| Elongation at break | 11%sourcetypical, longitudinal |
| Young's modulus (stiffness) | 70.3GPasourcetypical |
| Density | 2,830kg/m³sourcenominal |
| Strength to weight | 166kN·m/kg |
| Stiffness to weight | 24.8MN·m/kg |
| Poisson's ratio | 0.33sourcetypical (handbook physical constant) |
| Shear modulus | 26.4GPa |
| Bulk modulus | 68.9GPa |
| Speed of sound | 4,984m/s |
| Thermal | |
| Thermal conductivity | 157W/m·Ksourcetypical, 20 °C |
| Thermal expansion | 23.5µm/m·Ksourcetypical, mean 20-100 °C |
| 100 mm part over a 50 °C swing | 118µm growth |
| Specific heat | 860J/kg·Ksourcetypical, at 100 °C |
| Heats up and cools (diffusivity) | 64.5mm²/s |
| Thermal shock resistance | 29,862W/m |
| Melting point | 524–635°Csourcemelting range |
| Values for | 7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J |
Among 72 materials
Compare Aluminum 7050-T7451 with
Other Aluminum
- Aluminum 7050-T7451 vs. Aluminum
- Aluminum 7050-T7451 vs. Aluminum 6061-T6
- Aluminum 7050-T7451 vs. Aluminum 7075-T6
- Aluminum 7050-T7451 vs. Aluminum 2024-T351
- Aluminum 7050-T7451 vs. Aluminum 5052-H32
- Aluminum 7050-T7451 vs. Aluminum A380
- Aluminum 7050-T7451 vs. Aluminum 6063-T6
- Aluminum 7050-T7451 vs. Aluminum 1100-O
- Aluminum 7050-T7451 vs. Aluminum ADC12
Closest alternatives
- Aluminum 7050-T7451 vs. Concrete
- Aluminum 7050-T7451 vs. DMLS AlSi10Mg Aluminum
- Aluminum 7050-T7451 vs. Titanium
- Aluminum 7050-T7451 vs. Titanium Ti-6Al-4V
- Aluminum 7050-T7451 vs. Magnesium AZ31B-H24
- Aluminum 7050-T7451 vs. DMLS Ti-6Al-4V ELI Titanium
- Aluminum 7050-T7451 vs. Zinc Zamak 3
- Aluminum 7050-T7451 vs. PCB Laminate FR-4