Materials / Compare

Aluminum 7050-T7451 vs. Titanium

Compare Aluminum 7050-T7451 vs. Titanium strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7050-T7451Wrought
TitaniumWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength469MPasourcetypical, longitudinal, 0.2% offset885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset
Ultimate tensile strength524MPasourcetypical, longitudinal940MPasourcetypical, plate, annealed
Elongation at break11%sourcetypical, longitudinal16%sourcetypical, in 2 in., plate annealed
Young's modulus (stiffness)70.3GPasourcetypical107–122GPasourcetypical range, 20 °C
Density2,830kg/m³sourcenominal1.57x lighter4,430kg/m³sourcenominal
Strength to weight166kN·m/kg200kN·m/kg21% higher
Stiffness to weight24.8MN·m/kg25.8MN·m/kg4% higher
Poisson's ratio0.33sourcetypical (handbook physical constant)0.342sourcemean of TIMET measurements
Shear modulus26.4GPa42.7GPa1.61x stiffer in shear
Bulk modulus68.9GPa121GPa
Speed of sound4,984m/s5,084m/s
Thermal
Thermal conductivity157W/m·Ksourcetypical, 20 °C6.6W/m·Ksourcetypical, 20 °C, mill annealed
Thermal expansion23.5µm/m·Ksourcetypical, mean 20-100 °C9µm/m·Ksourcetypical, mean 0-100 °C
100 mm part over a 50 °C swing118µm growth45µm growth2.61x less
Specific heat860J/kg·Ksourcetypical, at 100 °C580J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)64.5mm²/s25.1x faster2.57mm²/s
Thermal shock resistance29,862W/m8.01x more resistant3,730W/m
Melting point524–635°Csourcemelting range1,630–1,650°Csourcemelting range
Max service temperaturenot sourced400°Csourceupper recommended use temperature
Values for7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5JTIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 7050-T7451 stronger than Titanium?

Titanium is stronger: its yield strength is 885 MPa against 469 MPa for Aluminum 7050-T7451 (1.89x).

Which is lighter, Aluminum 7050-T7451 or Titanium?

Aluminum 7050-T7451 is lighter: 2,830 kg/m³ against 4,430 kg/m³ for Titanium.

Which is stiffer, Aluminum 7050-T7451 or Titanium?

Titanium is stiffer: Young's modulus 115 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Titanium deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Titanium?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff beam (bending), stiff panel or plate, strong beam, strong panel or plate; Titanium is lighter for a stiff rod or tie (tension), strong rod or tie.

Part that must beAluminum 7050-T7451Titanium
Stiff rod or tie (tension)4% heavierlighter
Stiff beam (bending)lighter23% heavier
Stiff panel or platelighter33% heavier
Strong rod or tie21% heavierlighter
Strong beamlighter3% heavier
Strong panel or platelighter14% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 7050-T7451 or Titanium?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 6.6 W/m·K for Titanium.

Which expands less with temperature?

Titanium expands less: 9 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7050-T7451Titanium
Strength against density

Related comparisons