Mechanical
Yield strength324MPasourcetypical, 0.2% offset, .500 in dia specimen469MPasourcetypical, longitudinal, 0.2% offset
Ultimate tensile strength469MPasourcetypical524MPasourcetypical, longitudinal
Elongation at break19%sourcetypical, in 4D11%sourcetypical, longitudinal
Young's modulus (stiffness)73.1GPasourcetypical70.3GPasourcetypical
Density2,770kg/m³sourcenominal2,830kg/m³sourcenominal
Strength to weight117kN·m/kg166kN·m/kg42% higher
Stiffness to weight26.4MN·m/kg6% higher24.8MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant), all tempers0.33sourcetypical (handbook physical constant)
Shear modulus27.5GPa4% stiffer in shear26.4GPa
Bulk modulus71.7GPa68.9GPa
Speed of sound5,137m/s4,984m/s
Thermal
Thermal conductivity120W/m·Ksourcetypical, 20 °C157W/m·Ksourcetypical, 20 °C31% more heat through a fin
Thermal expansion22.9µm/m·Ksourcetypical, mean 20-100 °C23.5µm/m·Ksourcetypical, mean 20-100 °C
100 mm part over a 50 °C swing115µm growth3% less118µm growth
Specific heat875J/kg·Ksourcetypical, at 100 °C860J/kg·Ksourcetypical, at 100 °C
Heats up and cools (diffusivity)49.5mm²/s64.5mm²/s30% faster
Thermal shock resistance15,561W/m29,862W/m1.92x more resistant
Melting point502–638°Csourcemelting range524–635°Csourcemelting range
Values for2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5J

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 2024-T351 stronger than Aluminum 7050-T7451?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 324 MPa for Aluminum 2024-T351 (45%).

Which is lighter, Aluminum 2024-T351 or Aluminum 7050-T7451?

Aluminum 2024-T351 is lighter: 2,770 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.

Which is stiffer, Aluminum 2024-T351 or Aluminum 7050-T7451?

Aluminum 2024-T351 is stiffer: Young's modulus 73.1 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Aluminum 2024-T351 deflects less under the same load.

Which is lighter for the same job, Aluminum 2024-T351 or Aluminum 7050-T7451?

For the same stiffness or strength: Aluminum 2024-T351 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Aluminum 7050-T7451 is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 2024-T351Aluminum 7050-T7451
Stiff rod or tie (tension)lighter6% heavier
Stiff beam (bending)lighter4% heavier
Stiff panel or platelighter4% heavier
Strong rod or tie42% heavierlighter
Strong beam25% heavierlighter
Strong panel or plate18% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 2024-T351 or Aluminum 7050-T7451?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 120 W/m·K for Aluminum 2024-T351.

Which expands less with temperature?

Aluminum 2024-T351 expands less: 22.9 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 2024-T351Aluminum 7050-T7451
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 2024-T351Aluminum 7050-T7451
Strength against density

Related comparisons