Materials / Aluminum

Aluminum 2024-T351

Aluminum 2024-T351 (plate) strength, stiffness, density and thermal properties, with their source.

A bracket in Aluminum 2024-T351, brushed finish.

ProcessWrought
Mechanical
Yield strength324MPasourcetypical, 0.2% offset, .500 in dia specimen
Ultimate tensile strength469MPasourcetypical
Elongation at break19%sourcetypical, in 4D
Young's modulus (stiffness)73.1GPasourcetypical
Density2,770kg/m³sourcenominal
Strength to weight117kN·m/kg
Stiffness to weight26.4MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant), all tempers
Shear modulus27.5GPa
Bulk modulus71.7GPa
Speed of sound5,137m/s
Thermal
Thermal conductivity120W/m·Ksourcetypical, 20 °C
Thermal expansion22.9µm/m·Ksourcetypical, mean 20-100 °C
100 mm part over a 50 °C swing115µm growth
Specific heat875J/kg·Ksourcetypical, at 100 °C
Heats up and cools (diffusivity)49.5mm²/s
Thermal shock resistance15,561W/m
Melting point502–638°Csourcemelting range
Values for2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5J

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 2024-T351
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 2024-T351
Strength against density

Compare Aluminum 2024-T351 with