Aluminum 2024-T351Wrought
TitaniumWrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength324MPasourcetypical, 0.2% offset, .500 in dia specimen885MPasourcetypical, plate (>0.187 in), annealed, 0.2% offset
Ultimate tensile strength469MPasourcetypical940MPasourcetypical, plate, annealed
Elongation at break19%sourcetypical, in 4D16%sourcetypical, in 2 in., plate annealed
Young's modulus (stiffness)73.1GPasourcetypical107–122GPasourcetypical range, 20 °C
Density2,770kg/m³sourcenominal1.6x lighter4,430kg/m³sourcenominal
Strength to weight117kN·m/kg200kN·m/kg1.71x higher
Stiffness to weight26.4MN·m/kg2% higher25.8MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant), all tempers0.342sourcemean of TIMET measurements
Shear modulus27.5GPa42.7GPa1.55x stiffer in shear
Bulk modulus71.7GPa121GPa
Speed of sound5,137m/s5,084m/s
Thermal
Thermal conductivity120W/m·Ksourcetypical, 20 °C6.6W/m·Ksourcetypical, 20 °C, mill annealed
Thermal expansion22.9µm/m·Ksourcetypical, mean 20-100 °C9µm/m·Ksourcetypical, mean 0-100 °C
100 mm part over a 50 °C swing115µm growth45µm growth2.54x less
Specific heat875J/kg·Ksourcetypical, at 100 °C580J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)49.5mm²/s19.3x faster2.57mm²/s
Thermal shock resistance15,561W/m4.17x more resistant3,730W/m
Melting point502–638°Csourcemelting range1,630–1,650°Csourcemelting range
Max service temperaturenot sourced400°Csourceupper recommended use temperature
Values for2024-T4/T351, Kaiser Aluminum sheet, coil & plate typical datasheet; Poisson from MIL-HDBK-5JTIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 2024-T351 stronger than Titanium?

Titanium is stronger: its yield strength is 885 MPa against 324 MPa for Aluminum 2024-T351 (2.73x).

Which is lighter, Aluminum 2024-T351 or Titanium?

Aluminum 2024-T351 is lighter: 2,770 kg/m³ against 4,430 kg/m³ for Titanium.

Which is stiffer, Aluminum 2024-T351 or Titanium?

Titanium is stiffer: Young's modulus 115 GPa against 73.1 GPa for Aluminum 2024-T351, so the same part in Titanium deflects less under the same load.

Which is lighter for the same job, Aluminum 2024-T351 or Titanium?

For the same stiffness or strength: Aluminum 2024-T351 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Titanium is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 2024-T351Titanium
Stiff rod or tie (tension)lighter2% heavier
Stiff beam (bending)lighter28% heavier
Stiff panel or platelighter38% heavier
Strong rod or tie1.71x heavierlighter
Strong beam22% heavierlighter
Strong panel or plate3% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 2024-T351 or Titanium?

Aluminum 2024-T351 conducts heat better: 120 W/m·K against 6.6 W/m·K for Titanium.

Which expands less with temperature?

Titanium expands less: 9 µm/m·K against 22.9 µm/m·K for Aluminum 2024-T351.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 2024-T351Titanium
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 2024-T351Titanium
Strength against density