Aluminum 7050-T7451 vs. Magnesium AZ31B-H24

Compare Aluminum 7050-T7451 vs. Magnesium AZ31B-H24 strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7050-T7451Wrought
Magnesium AZ31B-H24Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength469MPasourcetypical, longitudinal, 0.2% offset220MPasourcetypical, H24, 0.5-6 mm, 0.2 % proof stress
Ultimate tensile strength524MPasourcetypical, longitudinal290MPasourcetypical, H24, 0.5-6 mm
Elongation at break11%sourcetypical, longitudinal13%sourcetypical, H24, 0.5-6 mm, gauge 5.65√A
Young's modulus (stiffness)70.3GPasourcetypical44.8GPasourcetypical (handbook physical constant)
Density2,830kg/m³sourcenominal1,769kg/m³sourcenominal1.6x lighter
Strength to weight166kN·m/kg33% higher124kN·m/kg
Stiffness to weight24.8MN·m/kg25.3MN·m/kg2% higher
Poisson's ratio0.33sourcetypical (handbook physical constant)0.35sourcetypical (handbook physical constant)
Shear modulus26.4GPa1.59x stiffer in shear16.6GPa
Bulk modulus68.9GPa49.8GPa
Speed of sound4,984m/s5,032m/s
Thermal
Thermal conductivity157W/m·Ksourcetypical, 20 °C76.9W/m·Ksourcetypical (temper/temperature not stated)
Thermal expansion23.5µm/m·Ksourcetypical, mean 20-100 °C26.8µm/m·Ksourcetypical (temperature range not stated)
100 mm part over a 50 °C swing118µm growth14% less134µm growth
Specific heat860J/kg·Ksourcetypical, at 100 °C1,040J/kg·Ksourcetypical
Heats up and cools (diffusivity)64.5mm²/s1.54x faster41.8mm²/s
Thermal shock resistance29,862W/m3.26x more resistant9,159W/m
Melting point524–635°Csourcemelting rangenot sourced
Max service temperaturenot sourced149°Csourcestated application limit
Values for7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5JAZ31B-H24 sheet 0.016-0.062 in., MIL-HDBK-5J Table 4.2.1.0(b) (AMS 4377); strengths are S-basis MINIMUMS

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 7050-T7451 stronger than Magnesium AZ31B-H24?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 220 MPa for Magnesium AZ31B-H24 (2.13x).

Which is lighter, Aluminum 7050-T7451 or Magnesium AZ31B-H24?

Magnesium AZ31B-H24 is lighter: 1,769 kg/m³ against 2,830 kg/m³ for Aluminum 7050-T7451.

Which is stiffer, Aluminum 7050-T7451 or Magnesium AZ31B-H24?

Aluminum 7050-T7451 is stiffer: Young's modulus 70.3 GPa against 44.8 GPa for Magnesium AZ31B-H24, so the same part in Aluminum 7050-T7451 deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Magnesium AZ31B-H24?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a strong rod or tie, strong beam; Magnesium AZ31B-H24 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong panel or plate.

Part that must beAluminum 7050-T7451Magnesium AZ31B-H24
Stiff rod or tie (tension)2% heavierlighter
Stiff beam (bending)28% heavierlighter
Stiff panel or plate38% heavierlighter
Strong rod or tielighter33% heavier
Strong beamlighter4% heavier
Strong panel or plate10% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 7050-T7451 or Magnesium AZ31B-H24?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 76.9 W/m·K for Magnesium AZ31B-H24.

Which expands less with temperature?

Aluminum 7050-T7451 expands less: 23.5 µm/m·K against 26.8 µm/m·K for Magnesium AZ31B-H24.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 7050-T7451Magnesium AZ31B-H24
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 7050-T7451Magnesium AZ31B-H24
Strength against density