Aluminum 7050-T7451 vs. Brass C360

Compare Aluminum 7050-T7451 vs. Brass C360 strength, stiffness, weight and thermal properties.

Change either side
Aluminum 7050-T7451Wrought
Brass C360Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength469MPasourcetypical, longitudinal, 0.2% offset310MPasourcetypical, 0.5% extension under load
Ultimate tensile strength524MPasourcetypical, longitudinal400MPasourcetypical
Elongation at break11%sourcetypical, longitudinal25%sourcetypical, 1 in. rod
Young's modulus (stiffness)70.3GPasourcetypical96.5GPasourcetypical, temper-independent
Density2,830kg/m³sourcenominal3x lighter8,498kg/m³sourcenominal
Strength to weight166kN·m/kg4.54x higher36.5kN·m/kg
Stiffness to weight24.8MN·m/kg2.19x higher11.4MN·m/kg
Poisson's ratio0.33sourcetypical (handbook physical constant)0.34sourcebase material: leaded free-machining brass CuZn39Pb2 (C37700), Wieland-Z30 rolled products, reference value at room temperature
Shear modulus26.4GPa36GPa36% stiffer in shear
Bulk modulus68.9GPa101GPa
Speed of sound4,984m/s3,370m/s
Thermal
Thermal conductivity157W/m·Ksourcetypical, 20 °C35% more heat through a fin116W/m·Ksourcetypical, 20 °C
Thermal expansion23.5µm/m·Ksourcetypical, mean 20-100 °C20.5µm/m·Ksourcetypical, mean 20-300 °C
100 mm part over a 50 °C swing118µm growth103µm growth15% less
Specific heat860J/kg·Ksourcetypical, at 100 °C377J/kg·Ksourcetypical, 20 °C
Heats up and cools (diffusivity)64.5mm²/s1.78x faster36.2mm²/s
Thermal shock resistance29,862W/m2.49x more resistant11,997W/m
Melting point524–635°Csourcemelting range888–899°Csourcesolidus-liquidus
Values for7050-T7451 plate, Kaiser Aluminum sheet, coil & plate typical datasheet (longitudinal); Poisson from MIL-HDBK-5JC36000 free-cutting brass, H02 half-hard rod 1 in. section (20% cold work), copper.org typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Aluminum 7050-T7451 stronger than Brass C360?

Aluminum 7050-T7451 is stronger: its yield strength is 469 MPa against 310 MPa for Brass C360 (1.51x).

Which is lighter, Aluminum 7050-T7451 or Brass C360?

Aluminum 7050-T7451 is lighter: 2,830 kg/m³ against 8,498 kg/m³ for Brass C360.

Which is stiffer, Aluminum 7050-T7451 or Brass C360?

Brass C360 is stiffer: Young's modulus 96.5 GPa against 70.3 GPa for Aluminum 7050-T7451, so the same part in Brass C360 deflects less under the same load.

Which is lighter for the same job, Aluminum 7050-T7451 or Brass C360?

For the same stiffness or strength: Aluminum 7050-T7451 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 7050-T7451Brass C360
Stiff rod or tie (tension)lighter2.19x heavier
Stiff beam (bending)lighter2.56x heavier
Stiff panel or platelighter2.7x heavier
Strong rod or tielighter4.54x heavier
Strong beamlighter3.96x heavier
Strong panel or platelighter3.69x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Aluminum 7050-T7451 or Brass C360?

Aluminum 7050-T7451 conducts heat better: 157 W/m·K against 116 W/m·K for Brass C360.

Which expands less with temperature?

Brass C360 expands less: 20.5 µm/m·K against 23.5 µm/m·K for Aluminum 7050-T7451.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelAluminum 7050-T7451Brass C360
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickAluminum 7050-T7451Brass C360
Strength against density