Materials / Compare

Brass C360 vs. Stainless Steel 304

Compare Brass C360 vs. Stainless Steel 304 strength, stiffness, weight and thermal properties.

Change either side
Brass C360Wrought
Stainless Steel 304Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength310MPasourcetypical, 0.5% extension under load241MPasourcetypical, annealed, 70 °F (21 °C)
Ultimate tensile strength400MPasourcetypical586MPasourcetypical, annealed, 70 °F (21 °C)
Elongation at break25%sourcetypical, 1 in. rod55%sourcetypical, annealed, in 2 in. (50.8 mm)
Young's modulus (stiffness)96.5GPasourcetypical, temper-independent193GPasourcetypical, in tension
Density8,498kg/m³sourcenominal8,030kg/m³sourcetypical
Strength to weight36.5kN·m/kg22% higher30kN·m/kg
Stiffness to weight11.4MN·m/kg24MN·m/kg2.12x higher
Poisson's ratio0.34sourcebase material: leaded free-machining brass CuZn39Pb2 (C37700), Wieland-Z30 rolled products, reference value at room temperature0.3sourcedesign value (structural stainless steels)
Shear modulus36GPa74.2GPa2.06x stiffer in shear
Bulk modulus101GPa161GPa
Speed of sound3,370m/s4,903m/s
Thermal
Thermal conductivity116W/m·Ksourcetypical, 20 °C16.2W/m·Ksourceat 100 °C
Thermal expansion20.5µm/m·Ksourcetypical, mean 20-300 °C16.9µm/m·Ksourcemean, 0–100 °C
100 mm part over a 50 °C swing103µm growth84.5µm growth21% less
Specific heat377J/kg·Ksourcetypical, 20 °C500J/kg·Ksourcemean, 0–100 °C
Heats up and cools (diffusivity)36.2mm²/s8.98x faster4.03mm²/s
Thermal shock resistance11,997W/m14.3x more resistant838W/m
Melting point888–899°Csourcesolidus-liquidus1,399–1,454°Csourcemelting range
Max service temperaturenot sourced899°Csourcecontinuous, oxidation (scaling) limit in air
Values forC36000 free-cutting brass, H02 half-hard rod 1 in. section (20% cold work), copper.org typical valuesType 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Brass C360 stronger than Stainless Steel 304?

Brass C360 is stronger: its yield strength is 310 MPa against 241 MPa for Stainless Steel 304 (29%).

Which is lighter, Brass C360 or Stainless Steel 304?

Stainless Steel 304 is lighter: 8,030 kg/m³ against 8,498 kg/m³ for Brass C360.

Which is stiffer, Brass C360 or Stainless Steel 304?

Stainless Steel 304 is stiffer: Young's modulus 193 GPa against 96.5 GPa for Brass C360, so the same part in Stainless Steel 304 deflects less under the same load.

Which is lighter for the same job, Brass C360 or Stainless Steel 304?

For the same stiffness or strength: Brass C360 is lighter for a strong rod or tie, strong beam, strong panel or plate; Stainless Steel 304 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beBrass C360Stainless Steel 304
Stiff rod or tie (tension)2.12x heavierlighter
Stiff beam (bending)50% heavierlighter
Stiff panel or plate33% heavierlighter
Strong rod or tielighter22% heavier
Strong beamlighter12% heavier
Strong panel or platelighter7% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Brass C360 or Stainless Steel 304?

Brass C360 conducts heat better: 116 W/m·K against 16.2 W/m·K for Stainless Steel 304.

Which expands less with temperature?

Stainless Steel 304 expands less: 16.9 µm/m·K against 20.5 µm/m·K for Brass C360.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrass C360Stainless Steel 304
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickBrass C360Stainless Steel 304
Strength against density

Related comparisons