Materials / Compare

Stainless Steel 304 vs. Stainless Steel 316

Compare Stainless Steel 304 vs. Stainless Steel 316 strength, stiffness, weight and thermal properties.

Change either side
Stainless Steel 304Wrought
Stainless Steel 316Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength241MPasourcetypical, annealed, 70 °F (21 °C)265MPasourcetypical (representative), annealed 1.0 mm sheet
Ultimate tensile strength586MPasourcetypical, annealed, 70 °F (21 °C)583MPasourcetypical (representative), annealed 1.0 mm sheet
Elongation at break55%sourcetypical, annealed, in 2 in. (50.8 mm)61%sourcetypical (representative), annealed, in 2 in. (51 mm)
Young's modulus (stiffness)193GPasourcetypical, in tension200GPasourcetypical, in tension
Density8,030kg/m³sourcetypical8,027kg/m³sourcetypical
Strength to weight30kN·m/kg33kN·m/kg10% higher
Stiffness to weight24MN·m/kg24.9MN·m/kg4% higher
Poisson's ratio0.3sourcedesign value (structural stainless steels)0.3sourcedesign value (structural stainless steels)
Shear modulus74.2GPa76.9GPa4% stiffer in shear
Bulk modulus161GPa167GPa
Speed of sound4,903m/s4,992m/s
Thermal
Thermal conductivity16.2W/m·Ksourceat 100 °C14.6W/m·Ksource20–100 °C
Thermal expansion16.9µm/m·Ksourcemean, 0–100 °C16.5µm/m·Ksourcemean, 20–100 °C
100 mm part over a 50 °C swing84.5µm growth82.5µm growth2% less
Specific heat500J/kg·Ksourcemean, 0–100 °C450J/kg·Ksourceat 20 °C
Heats up and cools (diffusivity)4.03mm²/s4.04mm²/s
Thermal shock resistance838W/m2% more resistant821W/m
Melting point1,399–1,454°Csourcemelting range1,390–1,440°Csourcemelting range
Max service temperature899°Csourcecontinuous, oxidation (scaling) limit in air871–899°Csourceoxidation (scaling) limit in air
Values forType 304, annealed flat-rolled (Cleveland-Cliffs 304/304L Product Data Bulletin, May 2021); Poisson's ratio from the Nickel Institute/SCI structural stainless design manualATI 316 (UNS S31600), annealed 1.0 mm sheet, ATI technical data sheet (2012); Poisson's ratio from the Nickel Institute/SCI structural stainless design manual

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Stainless Steel 304 stronger than Stainless Steel 316?

Stainless Steel 316 is stronger: its yield strength is 265 MPa against 241 MPa for Stainless Steel 304 (10%).

Which is lighter, Stainless Steel 304 or Stainless Steel 316?

Stainless Steel 316 is lighter: 8,027 kg/m³ against 8,030 kg/m³ for Stainless Steel 304.

Which is stiffer, Stainless Steel 304 or Stainless Steel 316?

Stainless Steel 316 is stiffer: Young's modulus 200 GPa against 193 GPa for Stainless Steel 304, so the same part in Stainless Steel 316 deflects less under the same load.

Which is lighter for the same job, Stainless Steel 304 or Stainless Steel 316?

For the same stiffness or strength: Stainless Steel 316 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beStainless Steel 304Stainless Steel 316
Stiff rod or tie (tension)4% heavierlighter
Stiff beam (bending)2% heavierlighter
Stiff panel or plate1% heavierlighter
Strong rod or tie10% heavierlighter
Strong beam7% heavierlighter
Strong panel or plate5% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Stainless Steel 304 or Stainless Steel 316?

Stainless Steel 304 conducts heat better: 16.2 W/m·K against 14.6 W/m·K for Stainless Steel 316.

Which expands less with temperature?

Stainless Steel 316 expands less: 16.5 µm/m·K against 16.9 µm/m·K for Stainless Steel 304.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelStainless Steel 304Stainless Steel 316
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickStainless Steel 304Stainless Steel 316
Strength against density

Related comparisons