Materials / Compare

Aluminum 7075-T6 vs. Steel AISI 4340

Compare Aluminum 7075-T6 vs. Steel AISI 4340 strength, stiffness, weight and thermal properties.

Aluminum 7075-T6Wrought
Steel AISI 4340Wrought
MechanicalAluminum 7075-T6Steel AISI 4340
Yield strength503MPa11,035MPa22.06x stronger
Ultimate tensile strength572MPa11,140MPa21.99x stronger
Elongation at break11%118%21.64x more ductile
Young's modulus (stiffness)71GPa1200GPa3
Density2,800kg/m³42.8x lighter7,840kg/m³2
Strength to weight180kN·m/kg36% higher132kN·m/kg
Stiffness to weight25.4MN·m/kg25.5MN·m/kg
Poisson's ratio0.3330.323
Shear modulus26.7GPa75.7GPa2.84x stiffer in shear
Bulk modulus69.6GPa185GPa2.66x higher
Speed of sound5,036m/s5,049m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Steel AISI 4340
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Steel AISI 4340
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum 7075-T6Steel AISI 4340
Thermal conductivity130W/m·K43.47x more heat through a fin37.5W/m·K2
Thermal expansion23.4µm/m·K4mean11.3µm/m·K22.07x less
100 mm part over a 50 °C swing117µm growth56.5µm growth2.07x less
Specific heat960J/kg·K42.14x higher448J/kg·K2
Heats up and cools (diffusivity)48.4mm²/s4.53x faster10.7mm²/s
Thermal shock resistance26,370W/m2.26x more resistant11,678W/m
Melting pointmelting range532–635°C4not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Steel AISI 4340
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum 7075-T6Steel AISI 4340
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Kaiser Aluminum, Carpenter Technology, U.S. Department of Defense
Aluminum 7075-T6
7075-T6/T651, Kaiser Aluminum rod & bar (mechanical) and sheet/coil/plate (physical) typical datasheets; Poisson from MIL-HDBK-5J
Steel AISI 4340
Carpenter (Latrobe) Lescalloy 4340 VAC-ARC datasheet; mechanical row for 1100 °F temper; physical properties grade-level
  1. 1
    Alloy 7075 Rod & Bar Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum 7075-T6 · Ultimate tensile strength: typicalAluminum 7075-T6 · Elongation at break: typical, in 4DAluminum 7075-T6 · Young's modulus (stiffness): typical
  2. 2
    Lescalloy 4340 VAC-ARC Data SheetCarpenter Technologyarchived copySteel AISI 4340 · Yield strength: typical, transverseSteel AISI 4340 · Ultimate tensile strength: typical, transverseSteel AISI 4340 · Elongation at break: typical, transverseSteel AISI 4340 · Density: typicalSteel AISI 4340 · Thermal conductivity: typicalSteel AISI 4340 · Thermal expansion: mean, -18 to 93 °CSteel AISI 4340 · Specific heat: typical
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Aluminum 7075-T6 · Poisson's ratio: typical (handbook physical constant)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
  4. 4
    Alloy 7075 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum 7075-T6 · Density: nominalAluminum 7075-T6 · Thermal conductivity: typical, 20 °C, T651Aluminum 7075-T6 · Thermal expansion: typical, mean 20-100 °CAluminum 7075-T6 · Specific heat: typical, at 100 °CAluminum 7075-T6 · Melting point: melting range

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum 7075-T6 stronger than Steel AISI 4340?

Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 503 MPa for Aluminum 7075-T6 (2.06x).

Which is lighter, Aluminum 7075-T6 or Steel AISI 4340?

Aluminum 7075-T6 is lighter: 2,800 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.

Which is stiffer, Aluminum 7075-T6 or Steel AISI 4340?

Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 71 GPa for Aluminum 7075-T6, so the same part in Steel AISI 4340 deflects less under the same load.

Which is lighter for the same job, Aluminum 7075-T6 or Steel AISI 4340?

For the same stiffness or strength: Aluminum 7075-T6 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beAluminum 7075-T6Steel AISI 4340
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)lighter1.67x heavier
Stiff panel or platelighter1.98x heavier
Strong rod or tielighter36% heavier
Strong beamlighter1.73x heavier
Strong panel or platelighter1.95x heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Aluminum 7075-T6 or Steel AISI 4340?

Steel AISI 4340 stretches further before it breaks: 18% elongation at break against 11% for Aluminum 7075-T6.

Thermal

Which conducts heat better, Aluminum 7075-T6 or Steel AISI 4340?

Aluminum 7075-T6 conducts heat better: 130 W/m·K against 37.5 W/m·K for Steel AISI 4340.

Which expands less with temperature?

Steel AISI 4340 expands less: 11.3 µm/m·K against 23.4 µm/m·K for Aluminum 7075-T6.

Related comparisons