Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
JIS ADC12 (Al-Si-Cu, about A383 / EN AC-46100) high-pressure die-casting alloy, as cast; physical properties from Daiki Aluminium Industry (ADC12 ingot producer) measured values; modulus from S.S.Aluminum (ADC12 ingot producer) standard values.
Drywall
1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittal
1
NA Alloys Product DataDaiki Aluminium IndustryAluminum ADC12 · Yield strength: one test result, 0.2% proof stress, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Ultimate tensile strength: one test result, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Elongation at break: one test result, as cast, ASTM tensile bar (Daiki)
2
Mechanical Properties of Gypsum Board at Elevated TemperaturesUSDA Forest Products LaboratoryDrywall · Ultimate tensile strength: ambient range reported in review (Australian studies)Drywall · Young's modulus (stiffness): ambient range reported in review (Australian studies)
3
GA-235-2023 Gypsum Board Typical Mechanical and Physical PropertiesGypsum AssociationDrywall · Compressive strength: typical, 70 F / 50% RHDrywall · Thermal expansion: typical, unrestrained, 3.3-32 CDrywall · Specific heat: typical (from ASHRAE Handbook of Fundamentals, per GA)
4
Die-Casting Alloys (ダイカスト用合金)S.S. AluminumAluminum ADC12 · Young's modulus (stiffness): standard value (S.S.Aluminum)
5
DIK365 Product DataDaiki Aluminium IndustryAluminum ADC12 · Density: measured (Daiki)Aluminum ADC12 · Thermal conductivity: measured on specimens cut from a 50 x 100 x 5 mm flat die casting (Daiki)Aluminum ADC12 · Thermal expansion: measured, temperature range not stated (Daiki)Aluminum ADC12 · Specific heat: measured (Daiki)Aluminum ADC12 · Melting point: solidus-liquidus (Daiki)
6
Sheetrock Brand UltraLight Panels Submittal Sheet (WB2501)USGarchived copyDrywall · Max service temperature: manufacturer sustained-exposure limit
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum ADC12 stronger than Drywall?
Aluminum ADC12 is stronger: its yield strength is 149 MPa against tensile strength 1.5 MPa for Drywall (99.3x).
Which is stiffer, Aluminum ADC12 or Drywall?
Aluminum ADC12 is stiffer: Young's modulus 79.8 GPa against 1.5 GPa for Drywall, so the same part in Aluminum ADC12 deflects less under the same load.
Thermal
Which expands less with temperature?
Drywall expands less: 16.7 µm/m·K against 21 µm/m·K for Aluminum ADC12.