Materials / Compare

Aluminum ADC12 vs. Plywood

Compare Aluminum ADC12 vs. Plywood strength, stiffness, weight and thermal properties.

Aluminum ADC12Cast
PlywoodNatural
MechanicalAluminum ADC12Plywood
Yield strengthone test result149MPa1not given (tensile used)
Ultimate tensile strengthone test result345MPa1modulus of rupture41.4MPa2
Flexural strengthnot sourcedstatic bending MOR41.4MPa2
Elongation at breakone test result2.3%1not sourced
Young's modulus (stiffness)standard value79.8GPa310.7x stiffer7.45GPa2
Densitymeasured2,680kg/m³4not sourced
Strength to weight55.6kN·m/kgnot sourced
Stiffness to weight29.8MN·m/kgnot sourced
Poisson's rationot sourcednot sourced
Shear modulusnot sourcednot sourced
Bulk modulusnot sourcednot sourced
Speed of sound5,457m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12
Strength against densityHigher and further left: stronger for its weight
ThermalAluminum ADC12Plywood
Thermal conductivity125W/m·K40.12W/m·K5
Thermal expansionmeasured21µm/m·K4base material3.1–4.5µm/m·K6
100 mm part over a 50 °C swing105µm growth19µm growth5.53x less
Specific heatmeasured911J/kg·K4base material1,700J/kg·K61.87x higher
Heats up and cools (diffusivity)51.2mm²/snot sourced
Thermal shock resistancenot sourcednot sourced
Melting pointsolidus-liquidus515–582°C4not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OMagnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum ADC12Plywood
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources6 documents: Daiki Aluminium Industry, USDA Forest Products Laboratory, S.S. Aluminum
Aluminum ADC12
JIS ADC12 (Al-Si-Cu, about A383 / EN AC-46100) high-pressure die-casting alloy, as cast; physical properties from Daiki Aluminium Industry (ADC12 ingot producer) measured values; modulus from S.S.Aluminum (ADC12 ingot producer) standard values.
Plywood
Douglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)
  1. 1
    NA Alloys Product DataDaiki Aluminium IndustryAluminum ADC12 · Yield strength: one test result, 0.2% proof stress, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Ultimate tensile strength: one test result, as cast, ASTM tensile bar (Daiki)Aluminum ADC12 · Elongation at break: one test result, as cast, ASTM tensile bar (Daiki)
  2. 2
    Wood Handbook (FPL-GTR-282), Chapter 12: Mechanical Properties of Wood-Based Composite MaterialsUSDA Forest Products LaboratoryPlywood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Plywood · Flexural strength: static bending MOR (Douglas-fir); range 33.72-42.61 across speciesPlywood · Young's modulus (stiffness): static bending MOE of the panel (Douglas-fir); range 6.96-8.55 across species
  3. 3
    Die-Casting Alloys (ダイカスト用合金)S.S. AluminumAluminum ADC12 · Young's modulus (stiffness): standard value (S.S.Aluminum)
  4. 4
    DIK365 Product DataDaiki Aluminium IndustryAluminum ADC12 · Density: measured (Daiki)Aluminum ADC12 · Thermal conductivity: measured on specimens cut from a 50 x 100 x 5 mm flat die casting (Daiki)Aluminum ADC12 · Thermal expansion: measured, temperature range not stated (Daiki)Aluminum ADC12 · Specific heat: measured (Daiki)Aluminum ADC12 · Melting point: solidus-liquidus (Daiki)
  5. 5
    Thermal Properties of Wood and Wood Panel Products for Use in Buildings (1988)USDA Forest Products Laboratoryarchived copyPlywood · Thermal conductivity: APA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL
  6. 6
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryPlywood · Thermal expansion: base material: solid wood parallel to grain, ovendry, range across speciesPlywood · Specific heat: base material: solid wood (all species), 12% MC, 27 C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Aluminum ADC12 stronger than Plywood?

Aluminum ADC12 is stronger: its yield strength is 149 MPa against tensile strength 41.4 MPa for Plywood (3.6x).

Which is stiffer, Aluminum ADC12 or Plywood?

Aluminum ADC12 is stiffer: Young's modulus 79.8 GPa against 7.45 GPa for Plywood, so the same part in Aluminum ADC12 deflects less under the same load.

Thermal

Which conducts heat better, Aluminum ADC12 or Plywood?

Aluminum ADC12 conducts heat better: 125 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Plywood expands less: 3.8 µm/m·K against 21 µm/m·K for Aluminum ADC12.

Related comparisons