Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
2
Ceramic Seal Material Properties (01899 F)CoorsTekarchived copyCeramic Alumina 96% · Ultimate tensile strength: typical tensile strength, 25 °C (ACMA Test #4)Ceramic Alumina 96% · Compressive strength: typical, 20 °C (ASTM-C773)Ceramic Alumina 96% · Flexural strength: flexural strength (MOR), 20 °C (ASTM-F417)Ceramic Alumina 96% · Young's modulus (stiffness): typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Density: typical (ASTM-C20)Ceramic Alumina 96% · Poisson's ratio: typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Thermal conductivity: typical, 20 °C (ASTM-C408)Ceramic Alumina 96% · Thermal expansion: mean, 25-1000 °C (ASTM-C372)Ceramic Alumina 96% · Specific heat: typical, 100 °C (ASTM-E1269)
3
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Aluminum stronger than Ceramic Alumina 96%?
Aluminum is stronger: its yield strength is 276 MPa against tensile strength 221 MPa for Ceramic Alumina 96% (25%).
Which is lighter, Aluminum or Ceramic Alumina 96%?
Aluminum is lighter: 2,700 kg/m³ against 3,720 kg/m³ for Ceramic Alumina 96%.
Which is stiffer, Aluminum or Ceramic Alumina 96%?
Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 68.3 GPa for Aluminum, so the same part in Ceramic Alumina 96% deflects less under the same load.
Which is lighter for the same job, Aluminum or Ceramic Alumina 96%?
For the same stiffness or strength: Aluminum is lighter for a strong rod or tie, strong beam, strong panel or plate; Ceramic Alumina 96% is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be
Aluminum
Ceramic Alumina 96%
Stiff rod or tie (tension)
3.22x heavier
lighter
Stiff beam (bending)
1.53x heavier
lighter
Stiff panel or plate
19% heavier
lighter
Strong rod or tie
lighter
1.72x heavier
Strong beam
lighter
1.6x heavier
Strong panel or plate
lighter
1.54x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Aluminum or Ceramic Alumina 96%?
Aluminum conducts heat better: 167 W/m·K against 24.7 W/m·K for Ceramic Alumina 96%.
Which expands less with temperature?
Ceramic Alumina 96% expands less: 8.2 µm/m·K against 23.6 µm/m·K for Aluminum.