Materials / Compare

Aluminum vs. Ceramic Aluminum Nitride

Compare Aluminum vs. Ceramic Aluminum Nitride strength, stiffness, weight and thermal properties.

AluminumWrought
Ceramic Aluminum NitrideSintered ceramic (pressed and fired)
MechanicalAluminumCeramic Aluminum Nitride
Yield strength276MPa1none (brittle)
Ultimate tensile strength310MPa1not sourced
Flexural strengthnot sourced310MPa2
Elongation at break17%1none (brittle)
Young's modulus (stiffness)68.3GPa1320GPa24.69x stiffer
Density2,700kg/m³126% lighter3,400kg/m³2
Strength to weight102kN·m/kgnot sourced
Stiffness to weight25.3MN·m/kg94.1MN·m/kg3.72x higher
Poisson's ratio0.3330.242
Shear modulus25.7GPa129GPa5.03x stiffer in shear
Bulk modulus67GPa205GPa3.06x higher
Speed of sound5,030m/s9,701m/s1.93x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumCeramic Aluminum Nitride
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Aluminum
Strength against densityHigher and further left: stronger for its weight
ThermalAluminumCeramic Aluminum Nitride
Thermal conductivity167W/m·K111% more heat through a fin150W/m·K2
Thermal expansion23.6µm/m·K1mean4.6µm/m·K25.13x less
100 mm part over a 50 °C swing118µm growth23µm growth5.13x less
Specific heat896J/kg·K126% higher710J/kg·K2
Heats up and cools (diffusivity)69mm²/s11% faster62.1mm²/s
Thermal shock resistance19,159W/mnot sourced
Melting pointsolidus-liquidus582–652°C1not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumCeramic Aluminum Nitride
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30AluminumCeramic Aluminum Nitride
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Kaiser Aluminum, KYOCERA Fineceramics Europe, U.S. Department of Defense
Aluminum
6061-T6/T651, Kaiser Aluminum typical properties (sheet, coil & plate datasheet); Poisson from MIL-HDBK-5J
Ceramic Aluminum Nitride
KYOCERA AN216A dense sintered aluminium nitride, typical values; KYOCERA Fineceramics Europe data sheet 2023.04.03
  1. 1
    Alloy 6061 Sheet, Coil & Plate Technical DataKaiser Aluminumarchived copyAluminum · Yield strength: typical, 0.2% offset, .500 in dia specimenAluminum · Ultimate tensile strength: typicalAluminum · Elongation at break: typical, in 4D, 0.500 in dia specimenAluminum · Young's modulus (stiffness): typicalAluminum · Density: nominalAluminum · Thermal conductivity: typical, 20 °CAluminum · Thermal expansion: typical, mean 20-100 °CAluminum · Specific heat: typical, at 100 °CAluminum · Melting point: solidus-liquidus
  2. 2
    AN216A Aluminium Nitride Data Sheet (2023)KYOCERA Fineceramics Europearchived copyCeramic Aluminum Nitride · Flexural strength: 3-point bending strength (JIS R 1601)Ceramic Aluminum Nitride · Young's modulus (stiffness): typical (JIS R 1602)Ceramic Aluminum Nitride · Density: typical (JIS R 1634)Ceramic Aluminum Nitride · Poisson's ratio: typical (JIS R 1602)Ceramic Aluminum Nitride · Thermal conductivity: typical (JIS R 1611)Ceramic Aluminum Nitride · Thermal expansion: mean, 40-400 °C (JIS R 1618)Ceramic Aluminum Nitride · Specific heat: typical (JIS R 1611)
  3. 3
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseAluminum · Poisson's ratio: typical (handbook physical constant)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Which is lighter, Aluminum or Ceramic Aluminum Nitride?

Aluminum is lighter: 2,700 kg/m³ against 3,400 kg/m³ for Ceramic Aluminum Nitride.

Which is stiffer, Aluminum or Ceramic Aluminum Nitride?

Ceramic Aluminum Nitride is stiffer: Young's modulus 320 GPa against 68.3 GPa for Aluminum, so the same part in Ceramic Aluminum Nitride deflects less under the same load.

Which is lighter for the same job, Aluminum or Ceramic Aluminum Nitride?

For the same stiffness or strength: Ceramic Aluminum Nitride is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beAluminumCeramic Aluminum Nitride
Stiff rod or tie (tension)3.72x heavierlighter
Stiff beam (bending)1.72x heavierlighter
Stiff panel or plate33% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Thermal

Which conducts heat better, Aluminum or Ceramic Aluminum Nitride?

Aluminum conducts heat better: 167 W/m·K against 150 W/m·K for Ceramic Aluminum Nitride.

Which expands less with temperature?

Ceramic Aluminum Nitride expands less: 4.6 µm/m·K against 23.6 µm/m·K for Aluminum.