Materials / Compare

Brass C260 vs. Steel AISI 4340

Compare Brass C260 vs. Steel AISI 4340 strength, stiffness, weight and thermal properties.

Brass C260Wrought
Steel AISI 4340Wrought
MechanicalBrass C260Steel AISI 4340
Yield strength345MPa11,035MPa23x stronger
Ultimate tensile strength427MPa11,140MPa22.67x stronger
Elongation at break23%128% more ductile18%2
Young's modulus (stiffness)110GPa3200GPa4
Density8,525kg/m³37,840kg/m³2
Strength to weight40.5kN·m/kg132kN·m/kg3.26x higher
Stiffness to weight12.9MN·m/kg25.5MN·m/kg1.97x higher
Poisson's ratio0.3450.324
Shear modulus41.2GPa75.7GPa1.84x stiffer in shear
Bulk modulus115GPa185GPa1.61x higher
Speed of sound3,597m/s5,049m/s40% faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260Steel AISI 4340
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260Steel AISI 4340
Strength against densityHigher and further left: stronger for its weight
ThermalBrass C260Steel AISI 4340
Thermal conductivity121W/m·K33.23x more heat through a fin37.5W/m·K2
Thermal expansion20µm/m·K3mean11.3µm/m·K21.77x less
100 mm part over a 50 °C swing100µm growth56.5µm growth1.77x less
Specific heat377J/kg·K3448J/kg·K219% higher
Heats up and cools (diffusivity)37.7mm²/s3.54x faster10.7mm²/s
Thermal shock resistance12,510W/m7% more resistant11,678W/m
Melting pointsolidus-liquidus916–954°C3not sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260Steel AISI 4340
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Brass C260Steel AISI 4340
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources5 documents: Copper Development Association, Carpenter Technology, U.S. Department of Defense, Wieland
Brass C260
C26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)
Steel AISI 4340
Carpenter (Latrobe) Lescalloy 4340 VAC-ARC datasheet; mechanical row for 1100 °F temper; physical properties grade-level
  1. 1
    Electronic Connector Design Guide: Cold Rolled TempersCopper Development Associationarchived copyBrass C260 · Yield strength: nominal, strip/flat, 0.5% extension (not 0.2% offset)Brass C260 · Ultimate tensile strength: nominal, strip/flatBrass C260 · Elongation at break: nominal, in 2.0 in., strip/flat
  2. 2
    Lescalloy 4340 VAC-ARC Data SheetCarpenter Technologyarchived copySteel AISI 4340 · Yield strength: typical, transverseSteel AISI 4340 · Ultimate tensile strength: typical, transverseSteel AISI 4340 · Elongation at break: typical, transverseSteel AISI 4340 · Density: typicalSteel AISI 4340 · Thermal conductivity: typicalSteel AISI 4340 · Thermal expansion: mean, -18 to 93 °CSteel AISI 4340 · Specific heat: typical
  3. 3
    C26000 Alloy (copper.org)Copper Development Associationarchived copyBrass C260 · Young's modulus (stiffness): typical, temper-independentBrass C260 · Density: nominalBrass C260 · Thermal conductivity: typical, 20 °CBrass C260 · Thermal expansion: typical, mean 20-300 °CBrass C260 · Specific heat: typical, 20 °CBrass C260 · Melting point: solidus-liquidus
  4. 4
    MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
  5. 5
    Wieland-M30 (CuZn30, C26000) Data SheetWielandarchived copyBrass C260 · Poisson's ratio: reference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Brass C260 stronger than Steel AISI 4340?

Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against 345 MPa for Brass C260 (3x).

Which is lighter, Brass C260 or Steel AISI 4340?

Steel AISI 4340 is lighter: 7,840 kg/m³ against 8,525 kg/m³ for Brass C260.

Which is stiffer, Brass C260 or Steel AISI 4340?

Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 110 GPa for Brass C260, so the same part in Steel AISI 4340 deflects less under the same load.

Which is lighter for the same job, Brass C260 or Steel AISI 4340?

For the same stiffness or strength: Steel AISI 4340 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beBrass C260Steel AISI 4340
Stiff rod or tie (tension)1.97x heavierlighter
Stiff beam (bending)46% heavierlighter
Stiff panel or plate33% heavierlighter
Strong rod or tie3.26x heavierlighter
Strong beam2.26x heavierlighter
Strong panel or plate1.88x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Brass C260 or Steel AISI 4340?

Brass C260 stretches further before it breaks: 23% elongation at break against 18% for Steel AISI 4340.

Thermal

Which conducts heat better, Brass C260 or Steel AISI 4340?

Brass C260 conducts heat better: 121 W/m·K against 37.5 W/m·K for Steel AISI 4340.

Which expands less with temperature?

Steel AISI 4340 expands less: 11.3 µm/m·K against 20 µm/m·K for Brass C260.