Brass C260Wrought
Zinc Zamak 3Cast
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength345MPasourcenominal, strip/flat, 0.5% extension (not 0.2% offset)221MPasourcetypical
Ultimate tensile strength427MPasourcenominal, strip/flat283MPasourcetypical
Elongation at break23%sourcenominal, in 2.0 in., strip/flat10%sourcetypical, in 2 in.
Young's modulus (stiffness)110GPasourcetypical, temper-independent85.5GPasourcetypical
Density8,525kg/m³sourcenominal6,600kg/m³sourcetypical
Strength to weight40.5kN·m/kg21% higher33.5kN·m/kg
Stiffness to weight12.9MN·m/kg13MN·m/kg
Poisson's ratio0.34sourcereference value at room temperature (Wieland-M30 = CuZn30 = C26000, rolled products)0.27sourcetypical, Zamak 3 hot-chamber die cast
Shear modulus41.2GPa22% stiffer in shear33.7GPa
Bulk modulus115GPa62GPa
Speed of sound3,597m/s3,599m/s
Thermal
Thermal conductivity121W/m·Ksourcetypical, 20 °C113W/m·Ksourcetypical
Thermal expansion20µm/m·Ksourcetypical, mean 20-300 °C27.4µm/m·Ksourcetypical
100 mm part over a 50 °C swing100µm growth37% less137µm growth
Specific heat377J/kg·Ksourcetypical, 20 °C419J/kg·Ksourcetypical
Heats up and cools (diffusivity)37.7mm²/s40.9mm²/s8% faster
Thermal shock resistance12,510W/m1.61x more resistant7,782W/m
Melting point916–954°Csourcesolidus-liquidus381–387°Csourcemelting range
Values forC26000 cartridge brass, H02 half hard flat/strip: CDA Electronic Connector Design Guide (mechanical) + CDA alloy page (physical)Zamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Brass C260 stronger than Zinc Zamak 3?

Brass C260 is stronger: its yield strength is 345 MPa against 221 MPa for Zinc Zamak 3 (1.56x).

Which is lighter, Brass C260 or Zinc Zamak 3?

Zinc Zamak 3 is lighter: 6,600 kg/m³ against 8,525 kg/m³ for Brass C260.

Which is stiffer, Brass C260 or Zinc Zamak 3?

Brass C260 is stiffer: Young's modulus 110 GPa against 85.5 GPa for Zinc Zamak 3, so the same part in Brass C260 deflects less under the same load.

Which is lighter for the same job, Brass C260 or Zinc Zamak 3?

For the same stiffness or strength: Brass C260 is lighter for a strong rod or tie, strong beam; Zinc Zamak 3 is lighter for a stiff beam (bending), stiff panel or plate, strong panel or plate.

Part that must beBrass C260Zinc Zamak 3
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)14% heavierlighter
Stiff panel or plate19% heavierlighter
Strong rod or tielighter21% heavier
Strong beamlighter4% heavier
Strong panel or plate3% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Brass C260 or Zinc Zamak 3?

Brass C260 conducts heat better: 121 W/m·K against 113 W/m·K for Zinc Zamak 3.

Which expands less with temperature?

Brass C260 expands less: 20 µm/m·K against 27.4 µm/m·K for Zinc Zamak 3.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrass C260Zinc Zamak 3
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VNickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickBrass C260Zinc Zamak 3
Strength against density

Related comparisons