Materials / Zinc

Zinc Zamak 3

Zinc Zamak 3 (die-cast) strength, stiffness, density and thermal properties, with their source.

A bracket in Zinc Zamak 3, as-cast finish.

ProcessCast
Mechanical
Yield strength221MPasourcetypical
Ultimate tensile strength283MPasourcetypical
Elongation at break10%sourcetypical, in 2 in.
Young's modulus (stiffness)85.5GPasourcetypical
Density6,600kg/m³sourcetypical
Strength to weight33.5kN·m/kg
Stiffness to weight13MN·m/kg
Poisson's ratio0.27sourcetypical, Zamak 3 hot-chamber die cast
Shear modulus33.7GPa
Bulk modulus62GPa
Speed of sound3,599m/s
Thermal
Thermal conductivity113W/m·Ksourcetypical
Thermal expansion27.4µm/m·Ksourcetypical
100 mm part over a 50 °C swing137µm growth
Specific heat419J/kg·Ksourcetypical
Heats up and cools (diffusivity)40.9mm²/s
Thermal shock resistance7,782W/m
Melting point381–387°Csourcemelting range
Values forZamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelZinc Zamak 3
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickZinc Zamak 3
Strength against density

Compare Zinc Zamak 3 with