Materials / Compare
Ceramic Alumina 96% vs. Concrete Compare Ceramic Alumina 96% vs. Concrete strength, stiffness, weight and thermal properties.
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Ceramic Alumina 96% Sintered ceramic (pressed and fired) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Concrete Cast Mechanical Ceramic Alumina 96% Concrete Yield strength none (brittle) none (brittle) Ultimate tensile strength 221 MPa not sourced Compressive strength 2,068 MPa 74.9x stronger in compression 27.6 MPa Flexural strength flexural strength 358 MPa not sourced Elongation at break none (brittle) none (brittle) Young's modulus (stiffness) 303 GPa design value 25.1 GPa Density 3,720 kg/m³ 2,240–2,400 kg/m³ Strength to weight 59.4 kN·m/kg not sourced Stiffness to weight 81.5 MN·m/kg 7.53x higher 10.8 MN·m/kg Poisson's ratio 0.21 0.15–0.2 Shear modulus 125 GPa 11.7x stiffer in shear 10.7 GPa Bulk modulus 174 GPa 13.5x higher 12.9 GPa Speed of sound 9,025 m/s 2.74x faster 3,289 m/s
1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel PCB Laminate FR-4 Silicon Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Ceramic Alumina 96% Concrete Stiffness against densityHigher and further left: stiffer for its weight 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Ceramic Alumina 96% Strength against densityHigher and further left: stronger for its weight
Thermal Ceramic Alumina 96% Concrete Thermal conductivity 24.7 W/m·K 27.4x more heat through a fin 0.9 W/m·K Thermal expansion mean 8.2 µm/m·K 8–12 µm/m·K 100 mm part over a 50 °C swing 41 µm growth 22% less 50 µm growth Specific heat 880 J/kg·K 900 J/kg·K Heats up and cools (diffusivity) 7.55 mm²/s 17.5x faster 0.431 mm²/s Thermal shock resistance 1,736 W/m not sourced Max service temperature not sourced 65 °C
1k 10k 0.1 1 10 100 Density (kg/m³) Thermal conductivity (W/m·K) Plastic PLA Plastic PETG Plastic ABS Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Ceramic Alumina 96% Concrete Thermal conductivity against densityHigher and further left: spreads more heat for its weight 0.1 1 10 100 10 100 Thermal conductivity (W/m·K) Thermal expansion (µm/m·K) Plastic PETG Plastic ABS Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel AISI 4340 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick Plywood PCB Laminate FR-4 Silicon Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Ceramic Alumina 96% Concrete Thermal expansion against thermal conductivityLower and further right: warps less when heated
Sources 8 documents: CoorsTek, National Ready Mixed Concrete Association, Federal Highway Administration, Oak Ridge National Laboratory, USDA Forest Products Laboratory, National Institute of Standards and Technology
Ceramic Alumina 96% CoorsTek AD-96, nominal 96% Al2O3 sintered alumina, typical values; CoorsTek "Ceramic Seal Material Properties" (© 2018, 01899 F). AD-96 is the general 96% grade, not the ADS-96R substrate grade.
Concrete Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review 1 Ceramic Seal Material Properties (01899 F) CoorsTek archived copy Ceramic Alumina 96% · Ultimate tensile strength: typical tensile strength, 25 °C (ACMA Test #4)Ceramic Alumina 96% · Compressive strength: typical, 20 °C (ASTM-C773)Ceramic Alumina 96% · Flexural strength: flexural strength (MOR), 20 °C (ASTM-F417)Ceramic Alumina 96% · Young's modulus (stiffness): typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Density: typical (ASTM-C20)Ceramic Alumina 96% · Poisson's ratio: typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Thermal conductivity: typical, 20 °C (ASTM-C408)Ceramic Alumina 96% · Thermal expansion: mean, 25-1000 °C (ASTM-C372)Ceramic Alumina 96% · Specific heat: typical, 100 °C (ASTM-E1269)2 CIP 35: Testing Compressive Strength of Concrete National Ready Mixed Concrete Association archived copy Concrete · Compressive strength: specified compressive strength class (f'c), not a measured typical3 LRFD Steel Girder Superstructure Bridge Design Example, Design Step 2: Concrete Deck Design Federal Highway Administration Concrete · Young's modulus (stiffness): design value: AASHTO LRFD 5.4.2.4 applied by FHWA to f'c = 4.0 ksi normal-weight concrete
4 CIP 36: Structural Lightweight Concrete National Ready Mixed Concrete Association archived copy Concrete · Density: range for normalweight concrete5 The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553) Oak Ridge National Laboratory archived copy Concrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)6 Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of Wood USDA Forest Products Laboratory Concrete · Thermal conductivity: typical (comparative value)
7 Thermal Coefficient of Portland Cement Concrete Federal Highway Administration Concrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
8 Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681) National Institute of Standards and Technology archived copy Concrete · Specific heat: typical (NIST guidance for thermal analysis)Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions Mechanical Which is lighter, Ceramic Alumina 96% or Concrete? Concrete is lighter: 2,320 kg/m³ against 3,720 kg/m³ for Ceramic Alumina 96%.
Which is stiffer, Ceramic Alumina 96% or Concrete? Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 25.1 GPa for Concrete, so the same part in Ceramic Alumina 96% deflects less under the same load.
Which is lighter for the same job, Ceramic Alumina 96% or Concrete? For the same stiffness or strength: Ceramic Alumina 96% is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.
Part that must be Ceramic Alumina 96% Concrete Stiff rod or tie (tension) lighter 7.53x heavier Stiff beam (bending) lighter 2.17x heavier Stiff panel or plate lighter 43% heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal Which conducts heat better, Ceramic Alumina 96% or Concrete? Ceramic Alumina 96% conducts heat better: 24.7 W/m·K against 0.9 W/m·K for Concrete.
Which expands less with temperature? Ceramic Alumina 96% expands less: 8.2 µm/m·K against 10 µm/m·K for Concrete.