Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sumitomo Chemical SUMIKASUPER LCP E6006L (30% glass fibre; high strength, low shrinkage); SUMIKASUPER LCP Technical Note, Version 04 / Nov. 2023, typical values.
1
Ceramic Seal Material Properties (01899 F)CoorsTekarchived copyCeramic Alumina 96% · Ultimate tensile strength: typical tensile strength, 25 °C (ACMA Test #4)Ceramic Alumina 96% · Compressive strength: typical, 20 °C (ASTM-C773)Ceramic Alumina 96% · Flexural strength: flexural strength (MOR), 20 °C (ASTM-F417)Ceramic Alumina 96% · Young's modulus (stiffness): typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Density: typical (ASTM-C20)Ceramic Alumina 96% · Poisson's ratio: typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Thermal conductivity: typical, 20 °C (ASTM-C408)Ceramic Alumina 96% · Thermal expansion: mean, 25-1000 °C (ASTM-C372)Ceramic Alumina 96% · Specific heat: typical, 100 °C (ASTM-E1269)
2
SUMIKASUPER LCP Technical Note, Version 04 (2023)Sumitomo Chemicalarchived copyPlastic LCP GF30 · Ultimate tensile strength: tensile strength (ISO 527)Plastic LCP GF30 · Flexural strength: typical (ISO 178)Plastic LCP GF30 · Elongation at break: tensile elongation (ISO 527)Plastic LCP GF30 · Young's modulus (stiffness): tensile modulus (ISO 527)Plastic LCP GF30 · Density: typicalPlastic LCP GF30 · Thermal conductivity: hot disk (ISO 22007-2), temperature not statedPlastic LCP GF30 · Thermal expansion: flow direction (MD), mean 50-150 °CPlastic LCP GF30 · Specific heat: ASTM E1269, temperature not statedPlastic LCP GF30 · Max service temperature: HDT 1.8 MPa (ISO 75)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Ceramic Alumina 96% stronger than Plastic LCP GF30?
Ceramic Alumina 96% is stronger: its tensile strength is 221 MPa against 115 MPa for Plastic LCP GF30 (1.92x).
Which is lighter, Ceramic Alumina 96% or Plastic LCP GF30?
Plastic LCP GF30 is lighter: 1,610 kg/m³ against 3,720 kg/m³ for Ceramic Alumina 96%.
Which is stiffer, Ceramic Alumina 96% or Plastic LCP GF30?
Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 11.5 GPa for Plastic LCP GF30, so the same part in Ceramic Alumina 96% deflects less under the same load.
Which is lighter for the same job, Ceramic Alumina 96% or Plastic LCP GF30?
For the same stiffness or strength: Ceramic Alumina 96% is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic LCP GF30 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Ceramic Alumina 96%
Plastic LCP GF30
Stiff rod or tie (tension)
lighter
11.4x heavier
Stiff beam (bending)
lighter
2.22x heavier
Stiff panel or plate
lighter
29% heavier
Strong rod or tie
20% heavier
lighter
Strong beam
49% heavier
lighter
Strong panel or plate
1.67x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Ceramic Alumina 96% or Plastic LCP GF30?
Ceramic Alumina 96% conducts heat better: 24.7 W/m·K against 0.5 W/m·K for Plastic LCP GF30.
Which expands less with temperature?
Ceramic Alumina 96% expands less: 8.2 µm/m·K against 20 µm/m·K for Plastic LCP GF30.