Ceramic Alumina 96%Sintered ceramic (pressed and fired)
PlywoodNatural
MechanicalCeramic Alumina 96%Plywood
Yield strengthnone (brittle)not given (tensile used)
Ultimate tensile strength221MPa1modulus of rupture41.4MPa2
Compressive strength2,068MPa1not sourced
Flexural strengthflexural strength358MPa1static bending MOR41.4MPa2
Elongation at breaknone (brittle)not sourced
Young's modulus (stiffness)303GPa140.7x stiffer7.45GPa2
Density3,720kg/m³1not sourced
Strength to weight59.4kN·m/kgnot sourced
Stiffness to weight81.5MN·m/kgnot sourced
Poisson's ratio0.211not sourced
Shear modulus125GPanot sourced
Bulk modulus174GPanot sourced
Speed of sound9,025m/snot sourced
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%
Strength against densityHigher and further left: stronger for its weight
ThermalCeramic Alumina 96%Plywood
Thermal conductivity24.7W/m·K10.12W/m·K3
Thermal expansionmean8.2µm/m·K1base material3.1–4.5µm/m·K4
100 mm part over a 50 °C swing41µm growth19µm growth2.16x less
Specific heat880J/kg·K1base material1,700J/kg·K41.93x higher
Heats up and cools (diffusivity)7.55mm²/snot sourced
Thermal shock resistance1,736W/mnot sourced
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Ceramic Alumina 96%Plywood
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA panel to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: CoorsTek, USDA Forest Products Laboratory
Ceramic Alumina 96%
CoorsTek AD-96, nominal 96% Al2O3 sintered alumina, typical values; CoorsTek "Ceramic Seal Material Properties" (© 2018, 01899 F). AD-96 is the general 96% grade, not the ADS-96R substrate grade.
Plywood
Douglas-fir plywood sheathing (construction plywood per PS 1), static bending properties from USDA FPL Wood Handbook FPL-GTR-282 Ch. 12 Table 12-2 (Biblis 2000)
  1. 1
    Ceramic Seal Material Properties (01899 F)CoorsTekarchived copyCeramic Alumina 96% · Ultimate tensile strength: typical tensile strength, 25 °C (ACMA Test #4)Ceramic Alumina 96% · Compressive strength: typical, 20 °C (ASTM-C773)Ceramic Alumina 96% · Flexural strength: flexural strength (MOR), 20 °C (ASTM-F417)Ceramic Alumina 96% · Young's modulus (stiffness): typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Density: typical (ASTM-C20)Ceramic Alumina 96% · Poisson's ratio: typical, 20 °C (ASTM-C848)Ceramic Alumina 96% · Thermal conductivity: typical, 20 °C (ASTM-C408)Ceramic Alumina 96% · Thermal expansion: mean, 25-1000 °C (ASTM-C372)Ceramic Alumina 96% · Specific heat: typical, 100 °C (ASTM-E1269)
  2. 2
    Wood Handbook (FPL-GTR-282), Chapter 12: Mechanical Properties of Wood-Based Composite MaterialsUSDA Forest Products LaboratoryPlywood · Ultimate tensile strength: modulus of rupture (no direct tensile value)Plywood · Flexural strength: static bending MOR (Douglas-fir); range 33.72-42.61 across speciesPlywood · Young's modulus (stiffness): static bending MOE of the panel (Douglas-fir); range 6.96-8.55 across species
  3. 3
    Thermal Properties of Wood and Wood Panel Products for Use in Buildings (1988)USDA Forest Products Laboratoryarchived copyPlywood · Thermal conductivity: APA-recommended design value (Douglas-fir plywood), as reported by FPL/ORNL
  4. 4
    Wood Handbook (FPL-GTR-282), Chapter 4: Moisture Relations and Physical Properties of WoodUSDA Forest Products LaboratoryPlywood · Thermal expansion: base material: solid wood parallel to grain, ovendry, range across speciesPlywood · Specific heat: base material: solid wood (all species), 12% MC, 27 C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Mechanical

Is Ceramic Alumina 96% stronger than Plywood?

Ceramic Alumina 96% is stronger: its tensile strength is 221 MPa against 41.4 MPa for Plywood (5.34x).

Which is stiffer, Ceramic Alumina 96% or Plywood?

Ceramic Alumina 96% is stiffer: Young's modulus 303 GPa against 7.45 GPa for Plywood, so the same part in Ceramic Alumina 96% deflects less under the same load.

Thermal

Which conducts heat better, Ceramic Alumina 96% or Plywood?

Ceramic Alumina 96% conducts heat better: 24.7 W/m·K against 0.12 W/m·K for Plywood.

Which expands less with temperature?

Plywood expands less: 3.8 µm/m·K against 8.2 µm/m·K for Ceramic Alumina 96%.