Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources9 documents: Carpenter Technology, National Ready Mixed Concrete Association, Federal Highway Administration, U.S. Department of Defense, Oak Ridge National Laboratory, USDA Forest Products Laboratory, National Institute of Standards and Technology
Concrete
Normal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC review
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
5
CIP 36: Structural Lightweight ConcreteNational Ready Mixed Concrete Associationarchived copyConcrete · Density: range for normalweight concrete
6
The Effect of Elevated Temperature on Concrete Materials and Structures: A Literature Review (ORNL/TM-2005/553)Oak Ridge National Laboratoryarchived copyConcrete · Poisson's ratio: general range at normal ambient conditions (overall 0.11-0.32)Concrete · Max service temperature: code long-term temperature limit (ASME Code, concrete containments)
Thermal Coefficient of Portland Cement ConcreteFederal Highway AdministrationConcrete · Thermal expansion: typical range for portland cement concrete (aggregate dependent)
9
Best Practice Guidelines for Structural Fire Resistance Design of Concrete and Steel Buildings (TN 1681)National Institute of Standards and Technologyarchived copyConcrete · Specific heat: typical (NIST guidance for thermal analysis)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Which is lighter, Concrete or Steel AISI 4340?
Concrete is lighter: 2,320 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is stiffer, Concrete or Steel AISI 4340?
Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 25.1 GPa for Concrete, so the same part in Steel AISI 4340 deflects less under the same load.
Which is lighter for the same job, Concrete or Steel AISI 4340?
For the same stiffness or strength: Concrete is lighter for a stiff beam (bending), stiff panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension).
Part that must be
Concrete
Steel AISI 4340
Stiff rod or tie (tension)
2.36x heavier
lighter
Stiff beam (bending)
lighter
20% heavier
Stiff panel or plate
lighter
1.69x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Concrete or Steel AISI 4340?
Steel AISI 4340 conducts heat better: 37.5 W/m·K against 0.9 W/m·K for Concrete.
Which expands less with temperature?
Concrete expands less: 10 µm/m·K against 11.3 µm/m·K for Steel AISI 4340.