Materials / Compare

Concrete vs. Zinc Zamak 3

Compare Concrete vs. Zinc Zamak 3 strength, stiffness, weight and thermal properties.

Change either side
ConcreteCast
Zinc Zamak 3Cast
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot sourced221MPasourcetypical
Ultimate tensile strengthnot sourced283MPasourcetypical
Compressive strength27.6MPasourcespecified compressive strength class (f'c), not a measured typicalnot sourced
Elongation at breaknot sourced10%sourcetypical, in 2 in.
Young's modulus (stiffness)not sourced85.5GPasourcetypical
Density2,240–2,400kg/m³sourcerange for normalweight concrete6,600kg/m³sourcetypical
Strength to weightnot sourced33.5kN·m/kg
Stiffness to weightnot sourced13MN·m/kg
Poisson's ratio0.15–0.2sourcegeneral range at normal ambient conditions (overall 0.11-0.32)0.27sourcetypical, Zamak 3 hot-chamber die cast
Shear modulusnot sourced33.7GPa
Bulk modulusnot sourced62GPa
Speed of soundnot sourced3,599m/s
Thermal
Thermal conductivity0.9W/m·Ksourcetypical (comparative value)113W/m·Ksourcetypical
Thermal expansion8–12µm/m·Ksourcetypical range for portland cement concrete (aggregate dependent)27.4µm/m·Ksourcetypical
100 mm part over a 50 °C swing50µm growth2.74x less137µm growth
Specific heat900J/kg·Ksourcetypical (NIST guidance for thermal analysis)419J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.431mm²/s40.9mm²/s94.9x faster
Thermal shock resistancenot sourced7,782W/m
Melting pointnot sourced381–387°Csourcemelting range
Max service temperature65°Csourcecode long-term temperature limit (ASME Code, concrete containments)not sourced
Values forNormal-weight portland cement concrete, strength class f'c = 4000 psi (28 MPa) per NRMCA CIP 35; density NRMCA CIP 36; thermal conductivity USDA FPL Wood Handbook; service temperature ORNL/NRC reviewZamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Which is lighter, Concrete or Zinc Zamak 3?

Concrete is lighter: 2,320 kg/m³ against 6,600 kg/m³ for Zinc Zamak 3.

Which conducts heat better, Concrete or Zinc Zamak 3?

Zinc Zamak 3 conducts heat better: 113 W/m·K against 0.9 W/m·K for Concrete.

Which expands less with temperature?

Concrete expands less: 10 µm/m·K against 27.4 µm/m·K for Zinc Zamak 3.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelZinc Zamak 3
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickZinc Zamak 3
Strength against density

Related comparisons