Materials / Compare

Copper C110 vs. Plastic TPU

Compare Copper C110 vs. Plastic TPU strength, stiffness, weight and thermal properties.

Copper C110Wrought
Plastic TPU3D printed (FDM)
MechanicalCopper C110Plastic TPU
Yield strength69MPa1not given (tensile used)
Ultimate tensile strength221MPa123.7MPa2
Flexural strengthnot sourced4.1MPa2
Elongation at break55%1not sourced
Young's modulus (stiffness)117GPa11,749x stiffer0.067GPa2
Density8,913kg/m³11,220kg/m³27.31x lighter
Strength to weight7.74kN·m/kg19.4kN·m/kg2.51x higher
Stiffness to weight13.1MN·m/kg239x higher0.0549MN·m/kg
Poisson's ratio0.343not sourced
Shear modulus43.7GPanot sourced
Bulk modulus122GPanot sourced
Speed of sound3,626m/s15.5x faster234m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic TPU
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110Plastic TPU
Strength against densityHigher and further left: stronger for its weight
ThermalCopper C110Plastic TPU
Thermal conductivity391W/m·K1not sourced
Thermal expansion16.9µm/m·K1not sourced
100 mm part over a 50 °C swing84.5µm growthnot sourced
Specific heat385J/kg·K1not sourced
Heats up and cools (diffusivity)114mm²/snot sourced
Thermal shock resistance8,992W/mnot sourced
Melting pointsolidus-liquidus1,065–1,083°C1217°C2
Max service temperaturenot sourcedHDT 0.455 MPa50.3°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Copper C110
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources3 documents: Copper Development Association, UltiMaker, Wieland
Copper C110
C11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical values
Plastic TPU
Ultimaker TPU 95A, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS (file v5.00), April 29, 2022.
  1. 1
    C11000 Alloy (copper.org)Copper Development Associationarchived copyCopper C110 · Yield strength: typical, 0.5% extension under loadCopper C110 · Ultimate tensile strength: typicalCopper C110 · Elongation at break: typical, 1 in. rodCopper C110 · Young's modulus (stiffness): typicalCopper C110 · Density: nominalCopper C110 · Thermal conductivity: typical, 20 °CCopper C110 · Thermal expansion: typical, mean 20-100 °CCopper C110 · Specific heat: typical, 20 °CCopper C110 · Melting point: solidus-liquidus
  2. 2
    Ultimaker TPU 95A Technical Data Sheet, v5.00UltiMakerarchived copyPlastic TPU · Ultimate tensile strength: typical, stress at breakPlastic TPU · Flexural strength: typicalPlastic TPU · Young's modulus (stiffness): typicalPlastic TPU · Density: typicalPlastic TPU · Melting point: typicalPlastic TPU · Max service temperature: HDT 0.455 MPa (printed specimens)
  3. 3
    Wieland-K32 (Cu-ETP, C11000) Data SheetWielandarchived copyCopper C110 · Poisson's ratio: reference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic TPU is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Copper C110 stronger than Plastic TPU?

Copper C110 is stronger: its yield strength is 69 MPa against tensile strength 23.7 MPa for Plastic TPU (2.91x).

Which is lighter, Copper C110 or Plastic TPU?

Plastic TPU is lighter: 1,220 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is stiffer, Copper C110 or Plastic TPU?

Copper C110 is stiffer: Young's modulus 117 GPa against 0.067 GPa for Plastic TPU, so the same part in Copper C110 deflects less under the same load.

Which is lighter for the same job, Copper C110 or Plastic TPU?

For the same stiffness or strength: Copper C110 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic TPU is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C110Plastic TPU
Stiff rod or tie (tension)lighter239x heavier
Stiff beam (bending)lighter5.72x heavier
Stiff panel or platelighter1.65x heavier
Strong rod or tie2.51x heavierlighter
Strong beam3.58x heavierlighter
Strong panel or plate4.28x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Related comparisons