Mechanical
Yield strength69MPasourcetypical, 0.5% extension under load221MPasourcetypical
Ultimate tensile strength221MPasourcetypical283MPasourcetypical28% stronger
Elongation at break55%sourcetypical, 1 in. rod10%sourcetypical, in 2 in.
Young's modulus (stiffness)117GPasourcetypical37% stiffer85.5GPasourcetypical
Density8,913kg/m³sourcenominal6,600kg/m³sourcetypical
Strength to weight7.74kN·m/kg33.5kN·m/kg4.33x higher
Stiffness to weight13.1MN·m/kg2% higher13MN·m/kg
Poisson's ratio0.34sourcereference value at room temperature (Wieland-K32 = Cu-ETP = C11000, rolled products)0.27sourcetypical, Zamak 3 hot-chamber die cast
Shear modulus43.7GPa30% stiffer in shear33.7GPa
Bulk modulus122GPa62GPa
Speed of sound3,626m/s3,599m/s
Thermal
Thermal conductivity391W/m·Ksourcetypical, 20 °C113W/m·Ksourcetypical
Thermal expansion16.9µm/m·Ksourcetypical, mean 20-100 °C27.4µm/m·Ksourcetypical
100 mm part over a 50 °C swing84.5µm growth1.62x less137µm growth
Specific heat385J/kg·Ksourcetypical, 20 °C419J/kg·Ksourcetypical
Heats up and cools (diffusivity)114mm²/s2.79x faster40.9mm²/s
Thermal shock resistance8,992W/m16% more resistant7,782W/m
Melting point1,065–1,083°Csourcesolidus-liquidus381–387°Csourcemelting range
Values forC11000 ETP copper, annealed to 0.050 mm grain size (OS050), 1 in. rod, copper.org typical valuesZamak 3 (ASTM B86 die cast), Nathan Trotter (zinc alloy producer) technical data sheet, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Copper C110 stronger than Zinc Zamak 3?

Zinc Zamak 3 is stronger: its yield strength is 221 MPa against 69 MPa for Copper C110 (3.2x).

Which is lighter, Copper C110 or Zinc Zamak 3?

Zinc Zamak 3 is lighter: 6,600 kg/m³ against 8,913 kg/m³ for Copper C110.

Which is stiffer, Copper C110 or Zinc Zamak 3?

Copper C110 is stiffer: Young's modulus 117 GPa against 85.5 GPa for Zinc Zamak 3, so the same part in Copper C110 deflects less under the same load.

Which is lighter for the same job, Copper C110 or Zinc Zamak 3?

For the same stiffness or strength: Copper C110 is lighter for a stiff rod or tie (tension); Zinc Zamak 3 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beCopper C110Zinc Zamak 3
Stiff rod or tie (tension)lighter2% heavier
Stiff beam (bending)15% heavierlighter
Stiff panel or plate22% heavierlighter
Strong rod or tie4.33x heavierlighter
Strong beam2.93x heavierlighter
Strong panel or plate2.42x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Copper C110 or Zinc Zamak 3?

Copper C110 conducts heat better: 391 W/m·K against 113 W/m·K for Zinc Zamak 3.

Which expands less with temperature?

Copper C110 expands less: 16.9 µm/m·K against 27.4 µm/m·K for Zinc Zamak 3.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelCopper C110Zinc Zamak 3
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickCopper C110Zinc Zamak 3
Strength against density

Related comparisons