Materials / Compare

DMLS 316L Stainless Steel vs. Steel AISI 1018

Compare DMLS 316L Stainless Steel vs. Steel AISI 1018 strength, stiffness, weight and thermal properties.

Change either side
DMLS 316L Stainless Steel3D printed metal (DMLS)
Steel AISI 1018Wrought
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength530MPasourcetypical, as manufactured, horizontal372MPasourceproducer-stated, cold drawn
Ultimate tensile strength640MPasourcetypical, as manufactured, horizontal441MPasourceproducer-stated, cold drawn
Elongation at break40%sourcetypical at break, as manufactured, horizontal15%sourcein 2 in (50.8 mm)
Young's modulus (stiffness)185GPasourcetypical, as built, horizontal (XY); EOSINT M280-400W / M290-400W, 316L_Surface 1.0, 20 µm (2014 sheet)200GPasourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Density7,900kg/m³sourcepart density (ISO 3369, not labelled min or typical), EOS M 290, 40 µm FlexLine7,861kg/m³sourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Strength to weight67.1kN·m/kg42% higher47.3kN·m/kg
Stiffness to weight23.4MN·m/kg25.4MN·m/kg9% higher
Poisson's ratio0.3sourcebase material: austenitic stainless steels incl. 1.4404 (316L), design value0.32sourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Shear modulus71.2GPa75.7GPa6% stiffer in shear
Bulk modulus154GPa185GPa
Speed of sound4,839m/s5,043m/s
Thermal
Thermal conductivity16.2W/m·Ksourcebase material: wrought 316/316L (Cleveland-Cliffs), at 100 °C51.9W/m·Ksourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Thermal expansion15.7µm/m·Ksourcemean 25-100 °C, ASTM E22812µm/m·Ksourcebase material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
100 mm part over a 50 °C swing78.6µm growth60µm growth31% less
Specific heat500J/kg·Ksourcebase material: wrought 316/316L (Cleveland-Cliffs), 0-100 °C486J/kg·Ksourcebase material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
Heats up and cools (diffusivity)4.1mm²/s13.6mm²/s3.31x faster
Thermal shock resistance2,067W/m5,473W/m2.65x more resistant
Values forEOS StainlessSteel 316L (powder 9011-0032), EOS M 290, ParameterSet 316L 20µm Surface M290/400W, as manufactured, horizontal; ISO 6892-1AISI 1018 cold drawn bar (Niagara LaSalle, cold-finished bar producer)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

DMLS 316L Stainless Steel is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is DMLS 316L Stainless Steel stronger than Steel AISI 1018?

DMLS 316L Stainless Steel is stronger: its yield strength is 530 MPa against 372 MPa for Steel AISI 1018 (42%).

Which is lighter, DMLS 316L Stainless Steel or Steel AISI 1018?

Steel AISI 1018 is lighter: 7,861 kg/m³ against 7,900 kg/m³ for DMLS 316L Stainless Steel.

Which is stiffer, DMLS 316L Stainless Steel or Steel AISI 1018?

Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 185 GPa for DMLS 316L Stainless Steel, so the same part in Steel AISI 1018 deflects less under the same load.

Which is lighter for the same job, DMLS 316L Stainless Steel or Steel AISI 1018?

For the same stiffness or strength: DMLS 316L Stainless Steel is lighter for a strong rod or tie, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate.

Part that must beDMLS 316L Stainless SteelSteel AISI 1018
Stiff rod or tie (tension)9% heavierlighter
Stiff beam (bending)4% heavierlighter
Stiff panel or plate3% heavierlighter
Strong rod or tielighter42% heavier
Strong beamlighter26% heavier
Strong panel or platelighter19% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, DMLS 316L Stainless Steel or Steel AISI 1018?

Steel AISI 1018 conducts heat better: 51.9 W/m·K against 16.2 W/m·K for DMLS 316L Stainless Steel.

Which expands less with temperature?

Steel AISI 1018 expands less: 12 µm/m·K against 15.7 µm/m·K for DMLS 316L Stainless Steel.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumStainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 17-4PH Stainless SteelDMLS 316L Stainless SteelSteel AISI 1018
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumStainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 17-4PH Stainless SteelBrickDMLS 316L Stainless SteelSteel AISI 1018
Strength against density

Related comparisons