Materials / Compare

Drywall vs. Plastic PEEK

Compare Drywall vs. Plastic PEEK strength, stiffness, weight and thermal properties.

Change either side
DrywallNatural
Plastic PEEKBulk polymer (molded or machined)
Try it on a partA sample part to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)98MPasourcetypical, tensile yield
Ultimate tensile strength1–2MPasourceambient range reported in review (Australian studies)not sourced
Compressive strength2.4MPasourcetypical, 70 F / 50% RH125MPasourcetypical, 23 C
Flexural strengthnot sourced165MPasourcetypical, flexural stress at yield, 23 C
Elongation at breaknot sourced25%sourcetypical, at break
Young's modulus (stiffness)1–2GPasourceambient range reported in review (Australian studies)4GPasourcetypical (nominal)
Densitynot sourced1,300kg/m³sourcetypical (crystalline)
Strength to weightnot sourced75.4kN·m/kg
Stiffness to weightnot sourced3.08MN·m/kg
Poisson's rationot sourced0.38sourcetypical
Shear modulusnot sourced1.45GPa
Bulk modulusnot sourced5.56GPa
Speed of soundnot sourced1,754m/s
Thermal
Thermal conductivitynot sourced0.29W/m·Ksourcetypical, average, 23 C
Thermal expansion16.7µm/m·Ksourcetypical, unrestrained, 3.3-32 C55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)
100 mm part over a 50 °C swing83.5µm growth3.29x less275µm growth
Specific heat1,090J/kg·Ksourcetypical (from ASHRAE Handbook of Fundamentals, per GA)2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Heats up and cools (diffusivity)not sourced0.101mm²/s
Thermal shock resistancenot sourced80.1W/m
Melting pointnot sourced343°Csourcetypical, DSC
Glass transitionnot sourced143°Csourceonset (midpoint 150 C)
Max service temperature52°Csourcemanufacturer sustained-exposure limit240°CsourceUL 746B RTI, mechanical strength (continuous use index)
Values for1/2 in. (12.7 mm) regular gypsum board (ASTM C1396), Gypsum Association GA-235-2019 typical/minimum properties; tensile and E from USDA FPL-co-authored review; service limit from USG Sheetrock 1/2 in. submittalVictrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Drywall stronger than Plastic PEEK?

Plastic PEEK is stronger: its yield strength is 98 MPa against tensile strength 1.5 MPa for Drywall (65.3x).

Which is stiffer, Drywall or Plastic PEEK?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 1.5 GPa for Drywall, so the same part in Plastic PEEK deflects less under the same load.

Which expands less with temperature?

Drywall expands less: 16.7 µm/m·K against 55 µm/m·K for Plastic PEEK.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PEEK
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless 304Stainless 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless 303Stainless 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PEEK
Strength against density

Related comparisons