Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003)U.S. Department of DefenseSteel AISI 1018 · Young's modulus (stiffness): base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Density: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Poisson's ratio: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Thermal conductivity: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)Steel AISI 1018 · Specific heat: base material: AISI 1025 plain carbon steel (MIL-HDBK-5J design value; ASTM A108 bar is the cold-finished carbon-steel bar spec that also covers 1018)
4
Luran S 777K (ASA) Product Data SheetINEOS StyrolutionFDM ASA · Thermal conductivity: base material: INEOS Styrolution Luran S 777K injection-molding ASA, typicalFDM ASA · Thermal expansion: base material: INEOS Styrolution Luran S 777K injection-molding ASA, range
5
S275JR Steel GradeOvakoSteel AISI 1018 · Thermal expansion: base material: unalloyed carbon steel, Ovako family table (S275JR, 'none alloyed structural steels', C <= 0.21%); mean 20-300 °C
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is FDM ASA stronger than Steel AISI 1018?
Steel AISI 1018 is stronger: its yield strength is 372 MPa against tensile strength 37 MPa for FDM ASA (10.1x).
Which is lighter, FDM ASA or Steel AISI 1018?
FDM ASA is lighter: 1,050 kg/m³ against 7,861 kg/m³ for Steel AISI 1018.
Which is stiffer, FDM ASA or Steel AISI 1018?
Steel AISI 1018 is stiffer: Young's modulus 200 GPa against 2.45 GPa for FDM ASA, so the same part in Steel AISI 1018 deflects less under the same load.
Which is lighter for the same job, FDM ASA or Steel AISI 1018?
For the same stiffness or strength: FDM ASA is lighter for a stiff panel or plate, strong beam, strong panel or plate; Steel AISI 1018 is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie.
Part that must be
FDM ASA
Steel AISI 1018
Stiff rod or tie (tension)
10.9x heavier
lighter
Stiff beam (bending)
21% heavier
lighter
Stiff panel or plate
lighter
1.73x heavier
Strong rod or tie
34% heavier
lighter
Strong beam
lighter
1.61x heavier
Strong panel or plate
lighter
2.36x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, FDM ASA or Steel AISI 1018?
Steel AISI 1018 stretches further before it breaks: 15% elongation at break against 9.2% for FDM ASA.
Thermal
Which conducts heat better, FDM ASA or Steel AISI 1018?
Steel AISI 1018 conducts heat better: 51.9 W/m·K against 0.17 W/m·K for FDM ASA.
Which expands less with temperature?
Steel AISI 1018 expands less: 12 µm/m·K against 95 µm/m·K for FDM ASA.