Materials / Compare

FDM ASA vs. Titanium

Compare FDM ASA vs. Titanium strength, stiffness, weight and thermal properties.

FDM ASA3D printed (FDM)
TitaniumWrought
MechanicalFDM ASATitanium
Yield strengthnot given (tensile used)885MPa1
Ultimate tensile strength37MPa2940MPa125.4x stronger
Flexural strength65MPa2not sourced
Elongation at break9.2%216%11.74x more ductile
Young's modulus (stiffness)2.45GPa2107–122GPa3
Density1,050kg/m³24.22x lighter4,430kg/m³1
Strength to weight35.2kN·m/kg200kN·m/kg5.67x higher
Stiffness to weight2.33MN·m/kg25.8MN·m/kg11.1x higher
Poisson's rationot sourced0.3421
Shear modulusnot sourced42.7GPa
Bulk modulusnot sourced121GPa
Speed of sound1,528m/s5,084m/s3.33x faster
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM ASATitanium
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM ASATitanium
Strength against densityHigher and further left: stronger for its weight
ThermalFDM ASATitanium
Thermal conductivitybase material0.17W/m·K46.6W/m·K338.8x more heat through a fin
Thermal expansionbase material80–110µm/m·K49µm/m·K3
100 mm part over a 50 °C swing475µm growth45µm growth10.6x less
Specific heatnot sourced580J/kg·K3
Heats up and cools (diffusivity)not sourced2.57mm²/s
Thermal shock resistancenot sourced3,730W/m
Melting pointnot sourcedmelting range1,630–1,650°C1
Max service temperatureHDT 1.8 MPa92°C2400°C1
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PLAPlastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM ASATitanium
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelIronSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30FDM ASATitanium
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: TIMET, Bambu Lab, INEOS Styrolution
FDM ASA
Bambu Lab ASA, TDS V3.0, printed specimens X-Y; nozzle 260 °C, bed 80 °C, 200 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.
Titanium
TIMETAL 6-4 (Ti-6Al-4V Grade 5) annealed plate typical (TIMET properties manual) + TIMET datasheet TMC-0150 physical properties
  1. 1
    TIMETAL 6-4 PropertiesTIMETarchived copyTitanium · Yield strength: typical, plate (>0.187 in), annealed, 0.2% offsetTitanium · Ultimate tensile strength: typical, plate, annealedTitanium · Elongation at break: typical, in 2 in., plate annealedTitanium · Density: nominalTitanium · Poisson's ratio: mean of TIMET measurementsTitanium · Melting point: melting rangeTitanium · Max service temperature: upper recommended use temperature
  2. 2
    Bambu ASA Technical Data Sheet, V3.0Bambu LabFDM ASA · Ultimate tensile strength: typicalFDM ASA · Flexural strength: typicalFDM ASA · Elongation at break: typicalFDM ASA · Young's modulus (stiffness): typicalFDM ASA · Density: typicalFDM ASA · Max service temperature: HDT 1.8 MPa
  3. 3
    TIMETAL 6-4 Data SheetTIMETarchived copyTitanium · Young's modulus (stiffness): typical range, 20 °CTitanium · Thermal conductivity: typical, 20 °C, mill annealedTitanium · Thermal expansion: typical, mean 0-100 °CTitanium · Specific heat: typical, 20 °C
  4. 4
    Luran S 777K (ASA) Product Data SheetINEOS StyrolutionFDM ASA · Thermal conductivity: base material: INEOS Styrolution Luran S 777K injection-molding ASA, typicalFDM ASA · Thermal expansion: base material: INEOS Styrolution Luran S 777K injection-molding ASA, range

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM ASA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is FDM ASA stronger than Titanium?

Titanium is stronger: its yield strength is 885 MPa against tensile strength 37 MPa for FDM ASA (23.9x).

Which is lighter, FDM ASA or Titanium?

FDM ASA is lighter: 1,050 kg/m³ against 4,430 kg/m³ for Titanium.

Which is stiffer, FDM ASA or Titanium?

Titanium is stiffer: Young's modulus 115 GPa against 2.45 GPa for FDM ASA, so the same part in Titanium deflects less under the same load.

Which is lighter for the same job, FDM ASA or Titanium?

For the same stiffness or strength: FDM ASA is lighter for a stiff panel or plate; Titanium is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM ASATitanium
Stiff rod or tie (tension)11.1x heavierlighter
Stiff beam (bending)1.62x heavierlighter
Stiff panel or platelighter17% heavier
Strong rod or tie5.67x heavierlighter
Strong beam1.97x heavierlighter
Strong panel or plate16% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, FDM ASA or Titanium?

Titanium stretches further before it breaks: 16% elongation at break against 9.2% for FDM ASA.

Thermal

Which conducts heat better, FDM ASA or Titanium?

Titanium conducts heat better: 6.6 W/m·K against 0.17 W/m·K for FDM ASA.

Which expands less with temperature?

Titanium expands less: 9 µm/m·K against 95 µm/m·K for FDM ASA.