Materials / Compare

FDM PAHT-CF vs. Plastic Polypropylene

Compare FDM PAHT-CF vs. Plastic Polypropylene strength, stiffness, weight and thermal properties.

Change either side
FDM PAHT-CF3D printed (FDM)
Plastic PolypropyleneBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)33MPasourcetypical, tensile stress at yield ISO 527
Ultimate tensile strength92MPasourcetypicalnot sourced
Flexural strength125MPasourcetypicalnot sourced
Elongation at break8.4%sourcetypicalnot sourced
Young's modulus (stiffness)3.86GPasourcetypical1.45GPasourcetypical, tensile modulus ISO 527
Density1,060kg/m³sourcetypical900kg/m³sourcetypical, 23 °C ISO 1183-1
Strength to weight86.8kN·m/kg2.37x higher36.7kN·m/kg
Stiffness to weight3.64MN·m/kg2.26x higher1.61MN·m/kg
Poisson's rationot sourced0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Shear modulusnot sourced0.511GPa
Bulk modulusnot sourced3.02GPa
Speed of sound1,908m/s1,269m/s
Thermal
Thermal conductivitynot sourced0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
Thermal expansionnot sourced80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene)
100 mm part over a 50 °C swingnot sourced450µm growth
Specific heatnot sourcednot sourced
Heats up and cools (diffusivity)not sourcednot sourced
Thermal shock resistancenot sourced28.6W/m
Melting point225°Csourcetypicalnot sourced
Glass transition70°Csourcetypicalnot sourced
Max service temperature170°CsourceHDT 1.8 MPa90°CsourceHDT 0.45 MPa (ISO 75B), unannealed
Values forBambu Lab PAHT-CF, TDS V3.0, printed specimens X-Y, dry state; nozzle 290 °C, bed 100 °C, 100 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM PAHT-CF is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM PAHT-CF stronger than Plastic Polypropylene?

FDM PAHT-CF is stronger: its tensile strength is 92 MPa against yield strength 33 MPa for Plastic Polypropylene (2.79x).

Which is lighter, FDM PAHT-CF or Plastic Polypropylene?

Plastic Polypropylene is lighter: 900 kg/m³ against 1,060 kg/m³ for FDM PAHT-CF.

Which is stiffer, FDM PAHT-CF or Plastic Polypropylene?

FDM PAHT-CF is stiffer: Young's modulus 3.86 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in FDM PAHT-CF deflects less under the same load.

Which is lighter for the same job, FDM PAHT-CF or Plastic Polypropylene?

For the same stiffness or strength: FDM PAHT-CF is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM PAHT-CFPlastic Polypropylene
Stiff rod or tie (tension)lighter2.26x heavier
Stiff beam (bending)lighter39% heavier
Stiff panel or platelighter18% heavier
Strong rod or tielighter2.37x heavier
Strong beamlighter1.68x heavier
Strong panel or platelighter42% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM PAHT-CFPlastic Polypropylene
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM PAHT-CFPlastic Polypropylene
Strength against density

Related comparisons