Materials / Compare

FDM PAHT-CF vs. Plastic PEEK

Compare FDM PAHT-CF vs. Plastic PEEK strength, stiffness, weight and thermal properties.

Change either side
FDM PAHT-CF3D printed (FDM)
Plastic PEEKBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)98MPasourcetypical, tensile yield
Ultimate tensile strength92MPasourcetypicalnot sourced
Compressive strengthnot sourced125MPasourcetypical, 23 C
Flexural strength125MPasourcetypical165MPasourcetypical, flexural stress at yield, 23 C
Elongation at break8.4%sourcetypical25%sourcetypical, at break
Young's modulus (stiffness)3.86GPasourcetypical4GPasourcetypical (nominal)
Density1,060kg/m³sourcetypical1,300kg/m³sourcetypical (crystalline)
Strength to weight86.8kN·m/kg15% higher75.4kN·m/kg
Stiffness to weight3.64MN·m/kg18% higher3.08MN·m/kg
Poisson's rationot sourced0.38sourcetypical
Shear modulusnot sourced1.45GPa
Bulk modulusnot sourced5.56GPa
Speed of sound1,908m/s1,754m/s
Thermal
Thermal conductivitynot sourced0.29W/m·Ksourcetypical, average, 23 C
Thermal expansionnot sourced55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)
100 mm part over a 50 °C swingnot sourced275µm growth
Specific heatnot sourced2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Heats up and cools (diffusivity)not sourced0.101mm²/s
Thermal shock resistancenot sourced80.1W/m
Melting point225°Csourcetypical343°Csourcetypical, DSC
Glass transition70°Csourcetypical143°Csourceonset (midpoint 150 C)
Max service temperature170°CsourceHDT 1.8 MPa240°CsourceUL 746B RTI, mechanical strength (continuous use index)
Values forBambu Lab PAHT-CF, TDS V3.0, printed specimens X-Y, dry state; nozzle 290 °C, bed 100 °C, 100 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

FDM PAHT-CF is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is FDM PAHT-CF stronger than Plastic PEEK?

Plastic PEEK is stronger: its yield strength is 98 MPa against tensile strength 92 MPa for FDM PAHT-CF (7%).

Which is lighter, FDM PAHT-CF or Plastic PEEK?

FDM PAHT-CF is lighter: 1,060 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, FDM PAHT-CF or Plastic PEEK?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 3.86 GPa for FDM PAHT-CF, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, FDM PAHT-CF or Plastic PEEK?

For the same stiffness or strength: FDM PAHT-CF is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beFDM PAHT-CFPlastic PEEK
Stiff rod or tie (tension)lighter18% heavier
Stiff beam (bending)lighter20% heavier
Stiff panel or platelighter21% heavier
Strong rod or tielighter15% heavier
Strong beamlighter18% heavier
Strong panel or platelighter19% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelFDM PAHT-CFPlastic PEEK
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickFDM PAHT-CFPlastic PEEK
Strength against density

Related comparisons