Materials / Compare

Plastic PEEK vs. Plastic PMMA

Compare Plastic PEEK vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Change either side
Plastic PEEKBulk polymer (molded or machined)
Plastic PMMABulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength98MPasourcetypical, tensile yieldnot given (tensile used)
Ultimate tensile strengthnot sourced80MPasourcetypical, 23 °C
Compressive strength125MPasourcetypical, 23 C110MPasourcecompressive yield stress, typical
Flexural strength165MPasourcetypical, flexural stress at yield, 23 C115MPasourcetypical
Elongation at break25%sourcetypical, at break5.5%sourcetypical
Young's modulus (stiffness)4GPasourcetypical (nominal)3.3GPasourcetypical, short-term
Density1,300kg/m³sourcetypical (crystalline)1,190kg/m³sourcetypical
Strength to weight75.4kN·m/kg12% higher67.2kN·m/kg
Stiffness to weight3.08MN·m/kg11% higher2.77MN·m/kg
Poisson's ratio0.38sourcetypical0.37sourcetypical
Shear modulus1.45GPa20% stiffer in shear1.2GPa
Bulk modulus5.56GPa4.23GPa
Speed of sound1,754m/s1,665m/s
Thermal
Thermal conductivity0.29W/m·Ksourcetypical, average, 23 C0.19W/m·Ksourcetypical
Thermal expansion55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing275µm growth27% less350µm growth
Specific heat2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.101mm²/s0.109mm²/s7% faster
Thermal shock resistance80.1W/m1.93x more resistant41.5W/m
Melting point343°Csourcetypical, DSCnot sourced
Glass transition143°Csourceonset (midpoint 150 C)not sourced
Max service temperature240°CsourceUL 746B RTI, mechanical strength (continuous use index)80°Csourcemax. permanent service temperature
Values forVictrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PEEK stronger than Plastic PMMA?

Plastic PEEK is stronger: its yield strength is 98 MPa against tensile strength 80 MPa for Plastic PMMA (23%).

Which is lighter, Plastic PEEK or Plastic PMMA?

Plastic PMMA is lighter: 1,190 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, Plastic PEEK or Plastic PMMA?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 3.3 GPa for Plastic PMMA, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, Plastic PEEK or Plastic PMMA?

For the same stiffness or strength: Plastic PEEK is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam, strong panel or plate; Plastic PMMA is lighter for a stiff panel or plate.

Part that must bePlastic PEEKPlastic PMMA
Stiff rod or tie (tension)lighter11% heavier
Stiff beam (bending)about equalabout equal
Stiff panel or plate2% heavierlighter
Strong rod or tielighter12% heavier
Strong beamlighter5% heavier
Strong panel or platelighter1% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PEEK or Plastic PMMA?

Plastic PEEK conducts heat better: 0.29 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Plastic PEEK expands less: 55 µm/m·K against 70 µm/m·K for Plastic PMMA.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic PEEKPlastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PEEKPlastic PMMA
Strength against density