Materials / Compare

Plastic Nylon PA6 vs. Plastic PEEK

Compare Plastic Nylon PA6 vs. Plastic PEEK strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA6Bulk polymer (molded or machined)
Plastic PEEKBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength90MPasourcetypical, dry98MPasourcetypical, tensile yield
Ultimate tensile strengthnot sourcednot sourced
Compressive strengthnot sourced125MPasourcetypical, 23 C
Flexural strengthnot sourced165MPasourcetypical, flexural stress at yield, 23 C
Elongation at break10%sourcenominal strain at break, dry25%sourcetypical, at break
Young's modulus (stiffness)3.5GPasourcetypical, dry4GPasourcetypical (nominal)
Density1,130kg/m³sourcetypical1,300kg/m³sourcetypical (crystalline)
Strength to weight79.6kN·m/kg6% higher75.4kN·m/kg
Stiffness to weight3.1MN·m/kg3.08MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.38sourcetypical
Shear modulus1.25GPa1.45GPa16% stiffer in shear
Bulk modulus5.83GPa5.56GPa
Speed of sound1,760m/s1,754m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypical0.29W/m·Ksourcetypical, average, 23 C
Thermal expansion102µm/m·Ksourcelongitudinal, 23-55 °C55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)
100 mm part over a 50 °C swing510µm growth275µm growth1.85x less
Specific heat1,700J/kg·Ksourcetypical2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)
Heats up and cools (diffusivity)0.172mm²/s1.69x faster0.101mm²/s
Thermal shock resistance49.9W/m80.1W/m1.6x more resistant
Melting point220°CsourceDSC343°Csourcetypical, DSC
Glass transitionnot sourced143°Csourceonset (midpoint 150 C)
Max service temperature87°CsourceIEC 60216 temperature index, 20000 h240°CsourceUL 746B RTI, mechanical strength (continuous use index)
Values forBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Victrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Nylon PA6 stronger than Plastic PEEK?

Plastic PEEK is stronger: its yield strength is 98 MPa against 90 MPa for Plastic Nylon PA6 (9%).

Which is lighter, Plastic Nylon PA6 or Plastic PEEK?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, Plastic Nylon PA6 or Plastic PEEK?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 3.5 GPa for Plastic Nylon PA6, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Plastic PEEK?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA6Plastic PEEK
Stiff rod or tie (tension)about equalabout equal
Stiff beam (bending)lighter8% heavier
Stiff panel or platelighter10% heavier
Strong rod or tielighter6% heavier
Strong beamlighter9% heavier
Strong panel or platelighter10% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon PA6 or Plastic PEEK?

Plastic Nylon PA6 conducts heat better: 0.33 W/m·K against 0.29 W/m·K for Plastic PEEK.

Which expands less with temperature?

Plastic PEEK expands less: 55 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6Plastic PEEK
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6Plastic PEEK
Strength against density