Materials / Compare

Plastic Nylon PA6 vs. Plastic PMMA

Compare Plastic Nylon PA6 vs. Plastic PMMA strength, stiffness, weight and thermal properties.

Change either side
Plastic Nylon PA6Bulk polymer (molded or machined)
Plastic PMMABulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength90MPasourcetypical, drynot given (tensile used)
Ultimate tensile strengthnot sourced80MPasourcetypical, 23 °C
Compressive strengthnot sourced110MPasourcecompressive yield stress, typical
Flexural strengthnot sourced115MPasourcetypical
Elongation at break10%sourcenominal strain at break, dry5.5%sourcetypical
Young's modulus (stiffness)3.5GPasourcetypical, dry3.3GPasourcetypical, short-term
Density1,130kg/m³sourcetypical1,190kg/m³sourcetypical
Strength to weight79.6kN·m/kg18% higher67.2kN·m/kg
Stiffness to weight3.1MN·m/kg12% higher2.77MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.37sourcetypical
Shear modulus1.25GPa4% stiffer in shear1.2GPa
Bulk modulus5.83GPa4.23GPa
Speed of sound1,760m/s1,665m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypical1.74x more heat through a fin0.19W/m·Ksourcetypical
Thermal expansion102µm/m·Ksourcelongitudinal, 23-55 °C70µm/m·Ksource0-50 °C
100 mm part over a 50 °C swing510µm growth350µm growth46% less
Specific heat1,700J/kg·Ksourcetypical1,470J/kg·Ksourcetypical
Heats up and cools (diffusivity)0.172mm²/s1.58x faster0.109mm²/s
Thermal shock resistance49.9W/m20% more resistant41.5W/m
Melting point220°CsourceDSCnot sourced
Max service temperature87°CsourceIEC 60216 temperature index, 20000 h80°Csourcemax. permanent service temperature
Values forBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Röhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Nylon PA6 stronger than Plastic PMMA?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against tensile strength 80 MPa for Plastic PMMA (13%).

Which is lighter, Plastic Nylon PA6 or Plastic PMMA?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,190 kg/m³ for Plastic PMMA.

Which is stiffer, Plastic Nylon PA6 or Plastic PMMA?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 3.3 GPa for Plastic PMMA, so the same part in Plastic Nylon PA6 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Plastic PMMA?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA6Plastic PMMA
Stiff rod or tie (tension)lighter12% heavier
Stiff beam (bending)lighter8% heavier
Stiff panel or platelighter7% heavier
Strong rod or tielighter18% heavier
Strong beamlighter14% heavier
Strong panel or platelighter12% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon PA6 or Plastic PMMA?

Plastic Nylon PA6 conducts heat better: 0.33 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Plastic PMMA expands less: 70 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6Plastic PMMA
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6Plastic PMMA
Strength against density

Related comparisons