Materials / Compare
FDM PAHT-CF vs. Steel AISI 4340 Compare FDM PAHT-CF vs. Steel AISI 4340 strength, stiffness, weight and thermal properties.
Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 FDM PAHT-CF 3D printed (FDM) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Rubber Wood Aluminum Aluminum 6061-T6 Aluminum 7075-T6 Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Steel Steel AISI 1018 Steel AISI 1045 Steel AISI 4340 Steel A992 Iron Titanium Titanium Ti-6Al-4V Stainless Steel 304 Stainless Steel 316 Stainless Steel 303 Stainless Steel 17-4PH Brass C360 Brass C260 Copper C110 Copper C10100 Copper C12200 Glass Nickel Inconel 718 Magnesium AZ31B-H24 Magnesium AZ91D Zinc Zamak 3 FDM ASA FDM Polycarbonate FDM PAHT-CF FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood Drywall PCB Laminate FR-4 PCB Board FR-4, 2 copper planes Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Solder SAC305 Steel AISI 4340 Wrought Mechanical FDM PAHT-CF Steel AISI 4340 Yield strength not given (tensile used) 1,035 MPa Ultimate tensile strength 92 MPa 1,140 MPa 12.4x stronger Flexural strength 125 MPa not sourced Elongation at break 8.4 % 18 % 2.14x more ductile Young's modulus (stiffness) 3.86 GPa 200 GPa Density 1,060 kg/m³ 7.4x lighter 7,840 kg/m³ Strength to weight 86.8 kN·m/kg 132 kN·m/kg 1.52x higher Stiffness to weight 3.64 MN·m/kg 25.5 MN·m/kg 7x higher Poisson's ratio not sourced 0.32 Shear modulus not sourced 75.7 GPa Bulk modulus not sourced 185 GPa Speed of sound 1,908 m/s 5,049 m/s 2.65x faster
1k 10k 0.1 1 10 100 Density (kg/m³) Young's modulus (GPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 FDM PAHT-CF Steel AISI 4340 Stiffness against densityHigher and further left: stiffer for its weight 1k 10k 10 100 1k Density (kg/m³) Yield strength (MPa) Plastic PLA Plastic PETG Plastic ABS Plastic TPU Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard SLA Resin Tough 2000 SLA Resin Elastic 50A SLS PA12 Nylon DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 FDM PAHT-CF Steel AISI 4340 Strength against densityHigher and further left: stronger for its weight
Thermal FDM PAHT-CF Steel AISI 4340 Thermal conductivity not sourced 37.5 W/m·K Thermal expansion not sourced mean 11.3 µm/m·K 100 mm part over a 50 °C swing not sourced 56.5 µm growth Specific heat not sourced 448 J/kg·K Heats up and cools (diffusivity) not sourced 10.7 mm²/s Thermal shock resistance not sourced 11,678 W/m Melting point 225 °C not sourced Glass transition 70 °C not sourced Max service temperature HDT 1.8 MPa 170 °C not sourced
1k 10k 0.1 1 10 100 Density (kg/m³) Thermal conductivity (W/m·K) Plastic PLA Plastic PETG Plastic ABS Plastic Nylon Rubber Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Steel AISI 4340 Thermal conductivity against densityHigher and further left: spreads more heat for its weight 0.1 1 10 100 10 100 Thermal conductivity (W/m·K) Thermal expansion (µm/m·K) Plastic PETG Plastic ABS Plastic Nylon Wood Aluminum Steel Iron Titanium Steel AISI 1018 Stainless Steel 304 Stainless Steel 316 Aluminum 6061-T6 Aluminum 7075-T6 Brass C360 Copper C110 Copper C10100 Copper C12200 Glass Steel AISI 1045 Steel A992 Stainless Steel 303 Stainless Steel 17-4PH Aluminum 2024-T351 Aluminum 5052-H32 Aluminum 7050-T7451 Titanium Ti-6Al-4V Brass C260 Nickel Inconel 718 Magnesium AZ31B-H24 Zinc Zamak 3 Plastic ABS (bulk/injection) Plastic Polycarbonate Plastic POM/Acetal Plastic Nylon PA6 Plastic Nylon PA66 Plastic PEEK Plastic PTFE Plastic UHMWPE Plastic HDPE Plastic Polypropylene Plastic PMMA FDM ASA FDM Polycarbonate FDM HIPS SLA Resin Standard DMLS AlSi10Mg Aluminum DMLS Ti-6Al-4V ELI Titanium DMLS 316L Stainless Steel DMLS 17-4PH Stainless Steel Concrete Brick Plywood PCB Laminate FR-4 Silicon Ceramic Alumina 96% Ceramic Aluminum Nitride Aluminum A380 Aluminum 6063-T6 Aluminum 1100-O Aluminum 3003-O Aluminum ADC12 Magnesium AZ91D Solder SAC305 Plastic PBT GF30 Plastic PPS GF40 Plastic LCP GF30 Steel AISI 4340 Thermal expansion against thermal conductivityLower and further right: warps less when heated
Sources 3 documents: Carpenter Technology, Bambu Lab, U.S. Department of Defense
FDM PAHT-CF Bambu Lab PAHT-CF, TDS V3.0, printed specimens X-Y, dry state; nozzle 290 °C, bed 100 °C, 100 mm/s, 100% infill; annealed and dried 80 °C for 12 h before testing.
Steel AISI 4340 Carpenter (Latrobe) Lescalloy 4340 VAC-ARC datasheet; mechanical row for 1100 °F temper; physical properties grade-level 1 Lescalloy 4340 VAC-ARC Data Sheet Carpenter Technology archived copy Steel AISI 4340 · Yield strength: typical, transverseSteel AISI 4340 · Ultimate tensile strength: typical, transverseSteel AISI 4340 · Elongation at break: typical, transverseSteel AISI 4340 · Density: typicalSteel AISI 4340 · Thermal conductivity: typicalSteel AISI 4340 · Thermal expansion: mean, -18 to 93 °CSteel AISI 4340 · Specific heat: typical2 Bambu PAHT-CF Technical Data Sheet, V3.0 Bambu Lab FDM PAHT-CF · Ultimate tensile strength: typicalFDM PAHT-CF · Flexural strength: typicalFDM PAHT-CF · Elongation at break: typicalFDM PAHT-CF · Young's modulus (stiffness): typicalFDM PAHT-CF · Density: typicalFDM PAHT-CF · Melting point: typicalFDM PAHT-CF · Glass transition: typicalFDM PAHT-CF · Max service temperature: HDT 1.8 MPa
3 MIL-HDBK-5J, Metallic Materials and Elements for Aerospace Vehicle Structures (2003) U.S. Department of Defense Steel AISI 4340 · Young's modulus (stiffness): MIL-HDBK-5J design value (AISI 4340, quenched and tempered)Steel AISI 4340 · Poisson's ratio: MIL-HDBK-5J design value (AISI 4340, quenched and tempered)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
FDM PAHT-CF is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions Mechanical Is FDM PAHT-CF stronger than Steel AISI 4340? Steel AISI 4340 is stronger: its yield strength is 1,035 MPa against tensile strength 92 MPa for FDM PAHT-CF (11.3x).
Which is lighter, FDM PAHT-CF or Steel AISI 4340? FDM PAHT-CF is lighter: 1,060 kg/m³ against 7,840 kg/m³ for Steel AISI 4340.
Which is stiffer, FDM PAHT-CF or Steel AISI 4340? Steel AISI 4340 is stiffer: Young's modulus 200 GPa against 3.86 GPa for FDM PAHT-CF, so the same part in Steel AISI 4340 deflects less under the same load.
Which is lighter for the same job, FDM PAHT-CF or Steel AISI 4340? For the same stiffness or strength: FDM PAHT-CF is lighter for a stiff beam (bending), stiff panel or plate, strong beam, strong panel or plate; Steel AISI 4340 is lighter for a stiff rod or tie (tension), strong rod or tie.
Part that must be FDM PAHT-CF Steel AISI 4340 Stiff rod or tie (tension) 7x heavier lighter Stiff beam (bending) lighter 3% heavier Stiff panel or plate lighter 1.98x heavier Strong rod or tie 1.52x heavier lighter Strong beam lighter 47% heavier Strong panel or plate lighter 2.21x heavier
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, FDM PAHT-CF or Steel AISI 4340? Steel AISI 4340 stretches further before it breaks: 18% elongation at break against 8.4% for FDM PAHT-CF.