Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA sample part to run stress or thermal on, free in your browser
Sources2 documents: Pilkington North America, Sumitomo Chemical
Glass
Annealed soda-lime-silica float glass, Pilkington North America Technical Bulletin ATS-129 (04/2025)
Plastic LCP GF30
Sumitomo Chemical SUMIKASUPER LCP E6006L (30% glass fibre; high strength, low shrinkage); SUMIKASUPER LCP Technical Note, Version 04 / Nov. 2023, typical values.
1
Technical Bulletin ATS-129: Properties of Soda-Lime Silica Float Glass (2025)Pilkington North Americaarchived copyGlass · Ultimate tensile strength: typical mean surface tensile stress at fracture (MOR), 60 s load, weathered, 50% breakage probabilityGlass · Flexural strength: mean MOR (same value as tensile)Glass · Young's modulus (stiffness): typicalGlass · Density: typicalGlass · Poisson's ratio: typicalGlass · Thermal conductivity: typical at 75 FGlass · Thermal expansion: typical, 75-575 FGlass · Specific heat: typical at 75 FGlass · Max service temperature: strain point (ASTM C336) - stress-relaxation onset, not a rated service limit
2
SUMIKASUPER LCP Technical Note, Version 04 (2023)Sumitomo Chemicalarchived copyPlastic LCP GF30 · Ultimate tensile strength: tensile strength (ISO 527)Plastic LCP GF30 · Flexural strength: typical (ISO 178)Plastic LCP GF30 · Elongation at break: tensile elongation (ISO 527)Plastic LCP GF30 · Young's modulus (stiffness): tensile modulus (ISO 527)Plastic LCP GF30 · Density: typicalPlastic LCP GF30 · Thermal conductivity: hot disk (ISO 22007-2), temperature not statedPlastic LCP GF30 · Thermal expansion: flow direction (MD), mean 50-150 °CPlastic LCP GF30 · Specific heat: ASTM E1269, temperature not statedPlastic LCP GF30 · Max service temperature: HDT 1.8 MPa (ISO 75)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Glass stronger than Plastic LCP GF30?
Plastic LCP GF30 is stronger: its tensile strength is 115 MPa against 41 MPa for Glass (2.8x).
Which is lighter, Glass or Plastic LCP GF30?
Plastic LCP GF30 is lighter: 1,610 kg/m³ against 2,500 kg/m³ for Glass.
Which is stiffer, Glass or Plastic LCP GF30?
Glass is stiffer: Young's modulus 72 GPa against 11.5 GPa for Plastic LCP GF30, so the same part in Glass deflects less under the same load.
Which is lighter for the same job, Glass or Plastic LCP GF30?
For the same stiffness or strength: Glass is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate; Plastic LCP GF30 is lighter for a strong rod or tie, strong beam, strong panel or plate.
Part that must be
Glass
Plastic LCP GF30
Stiff rod or tie (tension)
lighter
4.03x heavier
Stiff beam (bending)
lighter
1.61x heavier
Stiff panel or plate
lighter
19% heavier
Strong rod or tie
4.36x heavier
lighter
Strong beam
3.09x heavier
lighter
Strong panel or plate
2.6x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Thermal
Which conducts heat better, Glass or Plastic LCP GF30?
Glass conducts heat better: 0.937 W/m·K against 0.5 W/m·K for Plastic LCP GF30.
Which expands less with temperature?
Glass expands less: 8.3 µm/m·K against 20 µm/m·K for Plastic LCP GF30.