Materials / Compare

Iron vs. Plastic PLA

Compare Iron vs. Plastic PLA strength, stiffness, weight and thermal properties.

IronWrought
Plastic PLA3D printed (FDM)
MechanicalIronPlastic PLA
Yield strength186MPa13.54x stronger52.5MPa2
Ultimate tensile strength290MPa15.52x stronger52.5MPa2
Flexural strengthnot sourced96.8MPa2
Elongation at break38%14.87x more ductile7.8%2
Young's modulus (stiffness)207GPa163.7x stiffer3.25GPa2
Density7,860kg/m³11,240kg/m³26.34x lighter
Strength to weight23.7kN·m/kg42.3kN·m/kg1.79x higher
Stiffness to weight26.3MN·m/kg10x higher2.62MN·m/kg
Poisson's ratio0.2823not sourced
Shear modulus80.7GPanot sourced
Bulk modulus158GPanot sourced
Speed of sound5,132m/s3.17x faster1,619m/s
1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcretePCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PLA
Stiffness against densityHigher and further left: stiffer for its weight
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PETGPlastic ABSPlastic TPUPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin StandardSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PLA
Strength against densityHigher and further left: stronger for its weight
ThermalIronPlastic PLA
Thermal conductivity73.2W/m·K1563x more heat through a finbase material0.13W/m·K4
Thermal expansionmean13.7µm/m·K1not sourced
100 mm part over a 50 °C swing68.5µm growthnot sourced
Specific heat450J/kg·K1base material1,200J/kg·K42.67x higher
Heats up and cools (diffusivity)20.7mm²/s237x faster0.0874mm²/s
Thermal shock resistance3,447W/mnot sourced
Melting point1,532°C11,380 °C higher152°C2
Glass transitionnot sourced59.1°C2
Max service temperaturenot sourcedHDT 0.455 MPa58.8°C2
1k10k0.1110100Density (kg/m³)Thermal conductivity (W/m·K)Plastic PETGPlastic ABSPlastic NylonRubberWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30IronPlastic PLA
Thermal conductivity against densityHigher and further left: spreads more heat for its weight
0.111010010100Thermal conductivity (W/m·K)Thermal expansion (µm/m·K)Plastic PETGPlastic ABSPlastic NylonWoodAluminumSteelTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110Copper C10100Copper C12200GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic PolycarbonatePlastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM HIPSSLA Resin StandardDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelConcreteBrickPlywoodPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum 3003-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Iron
Thermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Sources4 documents: Cleveland-Cliffs, UltiMaker, National Institute of Standards and Technology, NatureWorks
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Plastic PLA
Ultimaker PLA, 3D-printed specimens, XY (flat) orientation; Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS dated April 20, 2022.
  1. 1
    ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
  2. 2
    Ultimaker PLA Technical Data Sheet, v5.00UltiMakerarchived copyPlastic PLA · Yield strength: typicalPlastic PLA · Ultimate tensile strength: typical, peak stress (= stress at yield)Plastic PLA · Flexural strength: typicalPlastic PLA · Elongation at break: typicalPlastic PLA · Young's modulus (stiffness): typicalPlastic PLA · Density: typicalPlastic PLA · Melting point: typicalPlastic PLA · Glass transition: typicalPlastic PLA · Max service temperature: HDT 0.455 MPa (printed specimens)
  3. 3
    Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
  4. 4
    Engineering Properties of Ingeo BiopolymerNatureWorksarchived copyPlastic PLA · Thermal conductivity: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °CPlastic PLA · Specific heat: base material: NatureWorks Ingeo biopolymer, amorphous sheet, 25 °C

Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic PLA is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Mechanical

Is Iron stronger than Plastic PLA?

Iron is stronger: its yield strength is 186 MPa against 52.5 MPa for Plastic PLA (3.54x).

Which is lighter, Iron or Plastic PLA?

Plastic PLA is lighter: 1,240 kg/m³ against 7,860 kg/m³ for Iron.

Which is stiffer, Iron or Plastic PLA?

Iron is stiffer: Young's modulus 207 GPa against 3.25 GPa for Plastic PLA, so the same part in Iron deflects less under the same load.

Which is lighter for the same job, Iron or Plastic PLA?

For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic PLA is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must beIronPlastic PLA
Stiff rod or tie (tension)lighter10x heavier
Stiff beam (bending)lighter26% heavier
Stiff panel or plate1.59x heavierlighter
Strong rod or tie1.79x heavierlighter
Strong beam2.73x heavierlighter
Strong panel or plate3.37x heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which is more ductile, Iron or Plastic PLA?

Iron stretches further before it breaks: 38% elongation at break against 7.8% for Plastic PLA.

Thermal

Which conducts heat better, Iron or Plastic PLA?

Iron conducts heat better: 73.2 W/m·K against 0.13 W/m·K for Plastic PLA.

Related comparisons