Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources5 documents: Cleveland-Cliffs, Covestro, National Institute of Standards and Technology, Bayer MaterialScience
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
Plastic Polycarbonate
Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values
1
ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
2
Makrolon 2405 Technical Data SheetCovestroPlastic Polycarbonate · Yield strength: typical, tensile yieldPlastic Polycarbonate · Ultimate tensile strength: typical, stress at breakPlastic Polycarbonate · Flexural strength: typical, flexural strengthPlastic Polycarbonate · Elongation at break: typical, strain at breakPlastic Polycarbonate · Young's modulus (stiffness): typicalPlastic Polycarbonate · Density: typicalPlastic Polycarbonate · Thermal conductivity: typical, through-plane, 23 CPlastic Polycarbonate · Thermal expansion: typical, 23-55 C, parallel and normalPlastic Polycarbonate · Glass transition: typical, DSC 10 C/minPlastic Polycarbonate · Max service temperature: UL 746B RTI, tensile strength, 1.5 mm
3
Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
4
Engineering Polymers Part and Mold Design: Thermoplastics, A Design GuideCovestroarchived copyPlastic Polycarbonate · Poisson's ratio: typical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
5
Makrolon 2405 Data Sheet, ASTM valuesBayer MaterialSciencearchived copyPlastic Polycarbonate · Specific heat: typical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Mechanical
Is Iron stronger than Plastic Polycarbonate?
Iron is stronger: its yield strength is 186 MPa against 65 MPa for Plastic Polycarbonate (2.86x).
Which is lighter, Iron or Plastic Polycarbonate?
Plastic Polycarbonate is lighter: 1,200 kg/m³ against 7,860 kg/m³ for Iron.
Which is stiffer, Iron or Plastic Polycarbonate?
Iron is stiffer: Young's modulus 207 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Iron deflects less under the same load.
Which is lighter for the same job, Iron or Plastic Polycarbonate?
For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending); Plastic Polycarbonate is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Iron
Plastic Polycarbonate
Stiff rod or tie (tension)
lighter
13.2x heavier
Stiff beam (bending)
lighter
42% heavier
Stiff panel or plate
48% heavier
lighter
Strong rod or tie
2.29x heavier
lighter
Strong beam
3.25x heavier
lighter
Strong panel or plate
3.87x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Iron or Plastic Polycarbonate?
Plastic Polycarbonate stretches further before it breaks: 125% elongation at break against 38% for Iron.
Thermal
Which conducts heat better, Iron or Plastic Polycarbonate?
Iron conducts heat better: 73.2 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.
Which expands less with temperature?
Iron expands less: 13.7 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.