Materials / Plastic

Plastic Polycarbonate

Plastic Polycarbonate (PC) strength, stiffness, density and thermal properties, with their source.

A bracket in Plastic Polycarbonate, smooth finish.

ProcessBulk polymer (molded or machined)
Mechanical
Yield strength65MPasourcetypical, tensile yield
Ultimate tensile strength65MPasourcetypical, stress at break
Flexural strength97MPasourcetypical, flexural strength
Elongation at break125%sourcetypical, strain at break
Young's modulus (stiffness)2.4GPasourcetypical
Density1,200kg/m³sourcetypical
Strength to weight54.2kN·m/kg
Stiffness to weight2MN·m/kg
Poisson's ratio0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
Shear modulus0.87GPa
Bulk modulus3.33GPa
Speed of sound1,414m/s
Thermal
Thermal conductivity0.2W/m·Ksourcetypical, through-plane, 23 C
Thermal expansion65µm/m·Ksourcetypical, 23-55 C, parallel and normal
100 mm part over a 50 °C swing325µm growth
Specific heat1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Heats up and cools (diffusivity)0.142mm²/s
Thermal shock resistance51.7W/m
Glass transition144°Csourcetypical, DSC 10 C/min
Max service temperature125°CsourceUL 746B RTI, tensile strength, 1.5 mm
Values forCovestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Polycarbonate
Strength against density