Materials / Compare

Plastic PEEK vs. Plastic Polycarbonate

Compare Plastic PEEK vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.

Change either side
Plastic PEEKBulk polymer (molded or machined)
Plastic PolycarbonateBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength98MPasourcetypical, tensile yield1.51x stronger65MPasourcetypical, tensile yield
Ultimate tensile strengthnot sourced65MPasourcetypical, stress at break
Compressive strength125MPasourcetypical, 23 Cnot sourced
Flexural strength165MPasourcetypical, flexural stress at yield, 23 C97MPasourcetypical, flexural strength
Elongation at break25%sourcetypical, at break125%sourcetypical, strain at break
Young's modulus (stiffness)4GPasourcetypical (nominal)2.4GPasourcetypical
Density1,300kg/m³sourcetypical (crystalline)1,200kg/m³sourcetypical
Strength to weight75.4kN·m/kg39% higher54.2kN·m/kg
Stiffness to weight3.08MN·m/kg1.54x higher2MN·m/kg
Poisson's ratio0.38sourcetypical0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
Shear modulus1.45GPa1.67x stiffer in shear0.87GPa
Bulk modulus5.56GPa3.33GPa
Speed of sound1,754m/s1,414m/s
Thermal
Thermal conductivity0.29W/m·Ksourcetypical, average, 23 C0.2W/m·Ksourcetypical, through-plane, 23 C
Thermal expansion55µm/m·Ksourceaverage of flow/cross-flow, below Tg (<143 C)65µm/m·Ksourcetypical, 23-55 C, parallel and normal
100 mm part over a 50 °C swing275µm growth18% less325µm growth
Specific heat2,200J/kg·Ksourcetypical, 23 °C, DSC (Victrex PEEK 450G TDS, revision Jul 2012)1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Heats up and cools (diffusivity)0.101mm²/s0.142mm²/s40% faster
Thermal shock resistance80.1W/m1.55x more resistant51.7W/m
Melting point343°Csourcetypical, DSCnot sourced
Glass transition143°Csourceonset (midpoint 150 C)144°Csourcetypical, DSC 10 C/min
Max service temperature240°CsourceUL 746B RTI, mechanical strength (continuous use index)125°CsourceUL 746B RTI, tensile strength, 1.5 mm
Values forVictrex PEEK 450G (unreinforced, injection moulded), Victrex TDS rev. March 2026; Poisson from Victrex fluid-management flyer (2020-07)Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PEEK stronger than Plastic Polycarbonate?

Plastic PEEK is stronger: its yield strength is 98 MPa against 65 MPa for Plastic Polycarbonate (1.51x).

Which is lighter, Plastic PEEK or Plastic Polycarbonate?

Plastic Polycarbonate is lighter: 1,200 kg/m³ against 1,300 kg/m³ for Plastic PEEK.

Which is stiffer, Plastic PEEK or Plastic Polycarbonate?

Plastic PEEK is stiffer: Young's modulus 4 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Plastic PEEK deflects less under the same load.

Which is lighter for the same job, Plastic PEEK or Plastic Polycarbonate?

For the same stiffness or strength: Plastic PEEK is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PEEKPlastic Polycarbonate
Stiff rod or tie (tension)lighter1.54x heavier
Stiff beam (bending)lighter19% heavier
Stiff panel or platelighter9% heavier
Strong rod or tielighter39% heavier
Strong beamlighter21% heavier
Strong panel or platelighter13% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PEEK or Plastic Polycarbonate?

Plastic PEEK conducts heat better: 0.29 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.

Which expands less with temperature?

Plastic PEEK expands less: 55 µm/m·K against 65 µm/m·K for Plastic Polycarbonate.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKPlastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PEEKPlastic Polycarbonate
Strength against density

Related comparisons