Materials / Compare

Plastic ABS vs. Plastic Polycarbonate

Compare Plastic ABS vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.

Change either side
Plastic ABS3D printed (FDM)
Plastic PolycarbonateBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength38.1MPasourcetypical65MPasourcetypical, tensile yield
Ultimate tensile strength38.1MPasourcetypical, peak stress (= stress at yield)65MPasourcetypical, stress at break
Flexural strength61.1MPasourcetypical97MPasourcetypical, flexural strength
Elongation at break4.6%sourcetypical125%sourcetypical, strain at break
Young's modulus (stiffness)1.96GPasourcetypical2.4GPasourcetypical22% stiffer
Density1,100kg/m³sourcetypical1,200kg/m³sourcetypical
Strength to weight34.6kN·m/kg54.2kN·m/kg1.56x higher
Stiffness to weight1.78MN·m/kg2MN·m/kg12% higher
Poisson's ratio0.39sourcebase material: ABS family typical (Covestro Part and Mold Design guide, Table 3-1)0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
Shear modulus0.706GPa0.87GPa23% stiffer in shear
Bulk modulus2.97GPa3.33GPa
Speed of sound1,336m/s1,414m/s
Thermal
Thermal conductivity0.17W/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, typical0.2W/m·Ksourcetypical, through-plane, 23 C
Thermal expansion80–110µm/m·Ksourcebase material: INEOS Styrolution Terluran GP-22 injection-molding ABS, range65µm/m·Ksourcetypical, 23-55 C, parallel and normal
100 mm part over a 50 °C swing475µm growth325µm growth46% less
Specific heatnot sourced1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Heats up and cools (diffusivity)not sourced0.142mm²/s
Thermal shock resistance21.2W/m51.7W/m2.44x more resistant
Glass transition101°Csourcetypical144°Csourcetypical, DSC 10 C/min
Max service temperature86.6°CsourceHDT 0.455 MPa (printed specimens)125°CsourceUL 746B RTI, tensile strength, 1.5 mm
Values forUltimaker ABS, 3D-printed specimens, XY (flat); Ultimaker S5 Pro, engineering intent profile, 0.15 mm layer height, AA 0.4 print core, 100% infill, Cura 4.9, printed one-at-a-time, conditioned >=24 h at room temperature. TDS v5.00, April 20, 2022.Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Plastic ABS is 3D printed: its properties depend on build direction and print settings; these are typical values.

Questions

Is Plastic ABS stronger than Plastic Polycarbonate?

Plastic Polycarbonate is stronger: its yield strength is 65 MPa against 38.1 MPa for Plastic ABS (1.71x).

Which is lighter, Plastic ABS or Plastic Polycarbonate?

Plastic ABS is lighter: 1,100 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.

Which is stiffer, Plastic ABS or Plastic Polycarbonate?

Plastic Polycarbonate is stiffer: Young's modulus 2.4 GPa against 1.96 GPa for Plastic ABS, so the same part in Plastic Polycarbonate deflects less under the same load.

Which is lighter for the same job, Plastic ABS or Plastic Polycarbonate?

For the same stiffness or strength: Plastic ABS is lighter for a stiff panel or plate; Plastic Polycarbonate is lighter for a stiff rod or tie (tension), stiff beam (bending), strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic ABSPlastic Polycarbonate
Stiff rod or tie (tension)12% heavierlighter
Stiff beam (bending)1% heavierlighter
Stiff panel or platelighter2% heavier
Strong rod or tie1.56x heavierlighter
Strong beam31% heavierlighter
Strong panel or plate20% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic ABS or Plastic Polycarbonate?

Plastic Polycarbonate conducts heat better: 0.2 W/m·K against 0.17 W/m·K for Plastic ABS.

Which expands less with temperature?

Plastic Polycarbonate expands less: 65 µm/m·K against 95 µm/m·K for Plastic ABS.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic ABSPlastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic ABSPlastic Polycarbonate
Strength against density