Materials / Compare

Plastic PMMA vs. Plastic Polycarbonate

Compare Plastic PMMA vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.

Change either side
Plastic PMMABulk polymer (molded or machined)
Plastic PolycarbonateBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strengthnot given (tensile used)65MPasourcetypical, tensile yield
Ultimate tensile strength80MPasourcetypical, 23 °C65MPasourcetypical, stress at break
Compressive strength110MPasourcecompressive yield stress, typicalnot sourced
Flexural strength115MPasourcetypical97MPasourcetypical, flexural strength
Elongation at break5.5%sourcetypical125%sourcetypical, strain at break
Young's modulus (stiffness)3.3GPasourcetypical, short-term2.4GPasourcetypical
Density1,190kg/m³sourcetypical1,200kg/m³sourcetypical
Strength to weight67.2kN·m/kg24% higher54.2kN·m/kg
Stiffness to weight2.77MN·m/kg39% higher2MN·m/kg
Poisson's ratio0.37sourcetypical0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
Shear modulus1.2GPa39% stiffer in shear0.87GPa
Bulk modulus4.23GPa3.33GPa
Speed of sound1,665m/s1,414m/s
Thermal
Thermal conductivity0.19W/m·Ksourcetypical0.2W/m·Ksourcetypical, through-plane, 23 C
Thermal expansion70µm/m·Ksource0-50 °C65µm/m·Ksourcetypical, 23-55 C, parallel and normal
100 mm part over a 50 °C swing350µm growth325µm growth8% less
Specific heat1,470J/kg·Ksourcetypical1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Heats up and cools (diffusivity)0.109mm²/s0.142mm²/s31% faster
Thermal shock resistance41.5W/m51.7W/m25% more resistant
Glass transitionnot sourced144°Csourcetypical, DSC 10 C/min
Max service temperature80°Csourcemax. permanent service temperature125°CsourceUL 746B RTI, tensile strength, 1.5 mm
Values forRöhm PLEXIGLAS GS 0F00 cast acrylic sheet, typical values at 23 °C / 50 % RH (Röhm Technical Information Ref. No. 211-1)Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic PMMA stronger than Plastic Polycarbonate?

Plastic PMMA is stronger: its tensile strength is 80 MPa against yield strength 65 MPa for Plastic Polycarbonate (23%).

Which is lighter, Plastic PMMA or Plastic Polycarbonate?

Plastic PMMA is lighter: 1,190 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.

Which is stiffer, Plastic PMMA or Plastic Polycarbonate?

Plastic PMMA is stiffer: Young's modulus 3.3 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Plastic PMMA deflects less under the same load.

Which is lighter for the same job, Plastic PMMA or Plastic Polycarbonate?

For the same stiffness or strength: Plastic PMMA is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PMMAPlastic Polycarbonate
Stiff rod or tie (tension)lighter39% heavier
Stiff beam (bending)lighter18% heavier
Stiff panel or platelighter12% heavier
Strong rod or tielighter24% heavier
Strong beamlighter16% heavier
Strong panel or platelighter12% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic PMMA or Plastic Polycarbonate?

Plastic Polycarbonate conducts heat better: 0.2 W/m·K against 0.19 W/m·K for Plastic PMMA.

Which expands less with temperature?

Plastic Polycarbonate expands less: 65 µm/m·K against 70 µm/m·K for Plastic PMMA.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PMMAPlastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropyleneFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic PMMAPlastic Polycarbonate
Strength against density

Related comparisons