| Mechanical | ||
| Yield strength | 65MPasourcetypical, tensile yield | 33MPasourcetypical, tensile stress at yield ISO 527 |
| Ultimate tensile strength | 65MPasourcetypical, stress at break | not sourced |
| Flexural strength | 97MPasourcetypical, flexural strength | not sourced |
| Elongation at break | 125%sourcetypical, strain at break | not sourced |
| Young's modulus (stiffness) | 2.4GPasourcetypical | 1.45GPasourcetypical, tensile modulus ISO 527 |
| Density | 1,200kg/m³sourcetypical | 900kg/m³sourcetypical, 23 °C ISO 1183-1 |
| Strength to weight | 54.2kN·m/kg48% higher | 36.7kN·m/kg |
| Stiffness to weight | 2MN·m/kg24% higher | 1.61MN·m/kg |
| Poisson's ratio | 0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1) | 0.42sourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene) |
| Shear modulus | 0.87GPa1.7x stiffer in shear | 0.511GPa |
| Bulk modulus | 3.33GPa | 3.02GPa |
| Speed of sound | 1,414m/s | 1,269m/s |
| Thermal | ||
| Thermal conductivity | 0.2W/m·Ksourcetypical, through-plane, 23 C | 0.17–0.22W/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene) |
| Thermal expansion | 65µm/m·Ksourcetypical, 23-55 C, parallel and normal | 80–100µm/m·Ksourcebase material: polypropylene homopolymer family (INEOS Olefins & Polymers USA, Typical Engineering Properties of Polypropylene) |
| 100 mm part over a 50 °C swing | 325µm growth38% less | 450µm growth |
| Specific heat | 1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766 | not sourced |
| Heats up and cools (diffusivity) | 0.142mm²/s | not sourced |
| Thermal shock resistance | 51.7W/m1.81x more resistant | 28.6W/m |
| Glass transition | 144°Csourcetypical, DSC 10 C/min | not sourced |
| Max service temperature | 125°CsourceUL 746B RTI, tensile strength, 1.5 mm | 90°CsourceHDT 0.45 MPa (ISO 75B), unannealed |
| Values for | Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values | LyondellBasell Moplen HP501H polypropylene homopolymer (general purpose), typical ISO values |
Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
Questions
Is Plastic Polycarbonate stronger than Plastic Polypropylene?
Plastic Polycarbonate is stronger: its yield strength is 65 MPa against 33 MPa for Plastic Polypropylene (1.97x).
Which is lighter, Plastic Polycarbonate or Plastic Polypropylene?
Plastic Polypropylene is lighter: 900 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.
Which is stiffer, Plastic Polycarbonate or Plastic Polypropylene?
Plastic Polycarbonate is stiffer: Young's modulus 2.4 GPa against 1.45 GPa for Plastic Polypropylene, so the same part in Plastic Polycarbonate deflects less under the same load.
Which is lighter for the same job, Plastic Polycarbonate or Plastic Polypropylene?
For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff rod or tie (tension), strong rod or tie, strong beam, strong panel or plate; Plastic Polypropylene is lighter for a stiff beam (bending), stiff panel or plate.
| Part that must be | Plastic Polycarbonate | Plastic Polypropylene |
|---|---|---|
| Stiff rod or tie (tension) | lighter | 24% heavier |
| Stiff beam (bending) | 4% heavier | lighter |
| Stiff panel or plate | 13% heavier | lighter |
| Strong rod or tie | lighter | 48% heavier |
| Strong beam | lighter | 18% heavier |
| Strong panel or plate | lighter | 5% heavier |
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which conducts heat better, Plastic Polycarbonate or Plastic Polypropylene?
Plastic Polycarbonate conducts heat better: 0.2 W/m·K against 0.195 W/m·K for Plastic Polypropylene.
Which expands less with temperature?
Plastic Polycarbonate expands less: 65 µm/m·K against 90 µm/m·K for Plastic Polypropylene.
Among 72 materials
Related comparisons
- Plastic Polycarbonate vs. Plastic Nylon
- Plastic Polycarbonate vs. SLA Resin Standard
- Plastic Polycarbonate vs. FDM Polycarbonate
- Plastic Polycarbonate vs. Plastic POM/Acetal
- Plastic Polypropylene vs. SLA Resin Tough 2000
- Plastic Polypropylene vs. Plastic ABS
- Plastic Polypropylene vs. SLS PA12 Nylon
- Plastic Polypropylene vs. Rubber