Materials / Compare

Plastic Polycarbonate vs. Rubber

Compare Plastic Polycarbonate vs. Rubber strength, stiffness, weight and thermal properties.

Change either side
Plastic PolycarbonateBulk polymer (molded or machined)
RubberBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength65MPasourcetypical, tensile yieldnot given (tensile used)
Ultimate tensile strength65MPasourcetypical, stress at break23MPasourcetypical
Flexural strength97MPasourcetypical, flexural strengthnot sourced
Elongation at break125%sourcetypical, strain at break830%sourcetypical
Young's modulus (stiffness)2.4GPasourcetypicalnot sourced
Density1,200kg/m³sourcetypical960kg/m³sourcetypical (specific gravity)
Strength to weight54.2kN·m/kg2.26x higher24kN·m/kg
Stiffness to weight2MN·m/kgnot sourced
Poisson's ratio0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)0.5sourcegovernment (NBS J. Res. 68A, 1964): computed by NBS for peroxide-cured gum NR vulcanizate, 25 °C, infinitesimal deformation0.49 in the solver: the linear element locks as the ratio nears 0.5 (nearly incompressible).
Shear modulus0.87GPanot sourced
Bulk modulus3.33GPanot sourced
Speed of sound1,414m/snot sourced
Thermal
Thermal conductivity0.2W/m·Ksourcetypical, through-plane, 23 C0.151W/m·Ksourcegovernment selected value (US Army Natick Laboratories TR 66-49-PR, 1966), soft vulcanized natural rubber, 25 °C
Thermal expansion65µm/m·Ksourcetypical, 23-55 C, parallel and normalnot sourced
100 mm part over a 50 °C swing325µm growthnot sourced
Specific heat1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 27661,881J/kg·Ksourcegovernment (NBS J. Res. 68A, Table 7; values observed for unvulcanized NR by Bekkedahl and Matheson), 25 °C
Heats up and cools (diffusivity)0.142mm²/s1.7x faster0.0836mm²/s
Thermal shock resistance51.7W/mnot sourced
Glass transition144°Csourcetypical, DSC 10 C/minnot sourced
Max service temperature125°CsourceUL 746B RTI, tensile strength, 1.5 mm70°Csourcecontinuous use operating range
Values forCovestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical valuesWeir Minerals Linatex Premium rubber (95 % natural rubber), typical physical properties, spec sheet WMD0118/202305

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Polycarbonate stronger than Rubber?

Plastic Polycarbonate is stronger: its yield strength is 65 MPa against tensile strength 23 MPa for Rubber (2.83x).

Which is lighter, Plastic Polycarbonate or Rubber?

Rubber is lighter: 960 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.

Which is lighter for the same job, Plastic Polycarbonate or Rubber?

For the same stiffness or strength: Plastic Polycarbonate is lighter for a strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic PolycarbonateRubber
Strong rod or tielighter2.26x heavier
Strong beamlighter1.6x heavier
Strong panel or platelighter34% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Polycarbonate or Rubber?

Plastic Polycarbonate conducts heat better: 0.2 W/m·K against 0.151 W/m·K for Rubber.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic PolycarbonateRubber
Strength against density

Related comparisons