Plastic Nylon PA6Bulk polymer (molded or machined)
Plastic PolycarbonateBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength90MPasourcetypical, dry65MPasourcetypical, tensile yield
Ultimate tensile strengthnot sourced65MPasourcetypical, stress at break
Flexural strengthnot sourced97MPasourcetypical, flexural strength
Elongation at break10%sourcenominal strain at break, dry125%sourcetypical, strain at break
Young's modulus (stiffness)3.5GPasourcetypical, dry2.4GPasourcetypical
Density1,130kg/m³sourcetypical1,200kg/m³sourcetypical
Strength to weight79.6kN·m/kg47% higher54.2kN·m/kg
Stiffness to weight3.1MN·m/kg1.55x higher2MN·m/kg
Poisson's ratio0.4sourcebase material: unfilled polyamide (PA), conditioned, maker design-guide family value (Covestro Table 3-1)0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
Shear modulus1.25GPa44% stiffer in shear0.87GPa
Bulk modulus5.83GPa3.33GPa
Speed of sound1,760m/s1,414m/s
Thermal
Thermal conductivity0.33W/m·Ksourcetypical0.2W/m·Ksourcetypical, through-plane, 23 C
Thermal expansion102µm/m·Ksourcelongitudinal, 23-55 °C65µm/m·Ksourcetypical, 23-55 C, parallel and normal
100 mm part over a 50 °C swing510µm growth325µm growth1.57x less
Specific heat1,700J/kg·Ksourcetypical1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Heats up and cools (diffusivity)0.172mm²/s21% faster0.142mm²/s
Thermal shock resistance49.9W/m51.7W/m4% more resistant
Melting point220°CsourceDSCnot sourced
Glass transitionnot sourced144°Csourcetypical, DSC 10 C/min
Max service temperature87°CsourceIEC 60216 temperature index, 20000 h125°CsourceUL 746B RTI, tensile strength, 1.5 mm
Values forBASF Ultramid B3S (PA6, unreinforced injection-moulding grade), Product Information 02/2026, dry values (ISO methods)Covestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic Nylon PA6 stronger than Plastic Polycarbonate?

Plastic Nylon PA6 is stronger: its yield strength is 90 MPa against 65 MPa for Plastic Polycarbonate (38%).

Which is lighter, Plastic Nylon PA6 or Plastic Polycarbonate?

Plastic Nylon PA6 is lighter: 1,130 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.

Which is stiffer, Plastic Nylon PA6 or Plastic Polycarbonate?

Plastic Nylon PA6 is stiffer: Young's modulus 3.5 GPa against 2.4 GPa for Plastic Polycarbonate, so the same part in Plastic Nylon PA6 deflects less under the same load.

Which is lighter for the same job, Plastic Nylon PA6 or Plastic Polycarbonate?

For the same stiffness or strength: Plastic Nylon PA6 is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic Nylon PA6Plastic Polycarbonate
Stiff rod or tie (tension)lighter1.55x heavier
Stiff beam (bending)lighter28% heavier
Stiff panel or platelighter20% heavier
Strong rod or tielighter47% heavier
Strong beamlighter32% heavier
Strong panel or platelighter25% heavier

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic Nylon PA6 or Plastic Polycarbonate?

Plastic Nylon PA6 conducts heat better: 0.33 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.

Which expands less with temperature?

Plastic Polycarbonate expands less: 65 µm/m·K against 102 µm/m·K for Plastic Nylon PA6.

Among 59 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPlastic Nylon PA6Plastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic HDPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPlastic Nylon PA6Plastic Polycarbonate
Strength against density

Related comparisons