Materials / Compare

Plastic HDPE vs. Plastic Polycarbonate

Compare Plastic HDPE vs. Plastic Polycarbonate strength, stiffness, weight and thermal properties.

Change either side
Plastic HDPEBulk polymer (molded or machined)
Plastic PolycarbonateBulk polymer (molded or machined)
Try it on a partA bracket to run stress or thermal on, free in your browserOpen in LessCADOpen in LessCAD
Mechanical
Yield strength24MPasourcetypical, tensile stress at yield 23 °C, 50 mm/min ISO 52765MPasourcetypical, tensile yield
Ultimate tensile strengthnot sourced65MPasourcetypical, stress at break
Flexural strengthnot sourced97MPasourcetypical, flexural strength
Elongation at breaknot sourced125%sourcetypical, strain at break
Young's modulus (stiffness)0.9GPasourcetypical, tensile modulus 23 °C ISO 5272.4GPasourcetypical
Density950kg/m³sourcetypical, ISO 11831,200kg/m³sourcetypical
Strength to weight25.3kN·m/kg54.2kN·m/kg2.14x higher
Stiffness to weight0.947MN·m/kg2MN·m/kg2.11x higher
Poisson's ratio0.4–0.45sourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)0.38sourcetypical, polycarbonate family (Covestro Part and Mold Design guide, Table 3-1)
Shear modulus0.316GPa0.87GPa2.75x stiffer in shear
Bulk modulus2GPa3.33GPa
Speed of sound973m/s1,414m/s
Thermal
Thermal conductivity0.4–0.49W/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)0.2W/m·Ksourcetypical, through-plane, 23 C
Thermal expansion120µm/m·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)65µm/m·Ksourcetypical, 23-55 C, parallel and normal
100 mm part over a 50 °C swing600µm growth325µm growth1.85x less
Specific heat2,250J/kg·Ksourcebase material: high-density polyethylene family (INEOS Olefins & Polymers USA, Typical Engineering Properties of HDPE)1,172J/kg·Ksourcetypical (guide value), Bayer ASTM datasheet for Makrolon 2405, ASTM D 2766
Heats up and cools (diffusivity)0.208mm²/s46% faster0.142mm²/s
Thermal shock resistance56.9W/m10% more resistant51.7W/m
Glass transitionnot sourced144°Csourcetypical, DSC 10 C/min
Max service temperaturenot sourced125°CsourceUL 746B RTI, tensile strength, 1.5 mm
Values forLyondellBasell Hostalen 23050 B high density polyethylene, typical ISO valuesCovestro Makrolon 2405 general-purpose PC (MVR 19), Covestro technical datasheet version 2026-09-28, typical values

Every value links to the document that states it. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.

Questions

Is Plastic HDPE stronger than Plastic Polycarbonate?

Plastic Polycarbonate is stronger: its yield strength is 65 MPa against 24 MPa for Plastic HDPE (2.71x).

Which is lighter, Plastic HDPE or Plastic Polycarbonate?

Plastic HDPE is lighter: 950 kg/m³ against 1,200 kg/m³ for Plastic Polycarbonate.

Which is stiffer, Plastic HDPE or Plastic Polycarbonate?

Plastic Polycarbonate is stiffer: Young's modulus 2.4 GPa against 0.9 GPa for Plastic HDPE, so the same part in Plastic Polycarbonate deflects less under the same load.

Which is lighter for the same job, Plastic HDPE or Plastic Polycarbonate?

For the same stiffness or strength: Plastic Polycarbonate is lighter for a stiff rod or tie (tension), stiff beam (bending), stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.

Part that must bePlastic HDPEPlastic Polycarbonate
Stiff rod or tie (tension)2.11x heavierlighter
Stiff beam (bending)29% heavierlighter
Stiff panel or plate10% heavierlighter
Strong rod or tie2.14x heavierlighter
Strong beam1.54x heavierlighter
Strong panel or plate30% heavierlighter

For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).

Which conducts heat better, Plastic HDPE or Plastic Polycarbonate?

Plastic HDPE conducts heat better: 0.445 W/m·K against 0.2 W/m·K for Plastic Polycarbonate.

Which expands less with temperature?

Plastic Polycarbonate expands less: 65 µm/m·K against 120 µm/m·K for Plastic HDPE.

Among 72 materials

1k10k0.1110100Density (kg/m³)Young's modulus (GPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelPCB Laminate FR-4SiliconCeramic Alumina 96%Ceramic Aluminum NitrideAluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic HDPEPlastic Polycarbonate
Stiffness against density
1k10k101001kDensity (kg/m³)Yield strength (MPa)Plastic PLAPlastic PETGPlastic ABSPlastic TPUPlastic NylonRubberAluminumSteelIronTitaniumSteel AISI 1018Stainless Steel 304Stainless Steel 316Aluminum 6061-T6Aluminum 7075-T6Brass C360Copper C110GlassSteel AISI 1045Steel AISI 4340Steel A992Stainless Steel 303Stainless Steel 17-4PHAluminum 2024-T351Aluminum 5052-H32Aluminum 7050-T7451Titanium Ti-6Al-4VBrass C260Nickel Inconel 718Magnesium AZ31B-H24Zinc Zamak 3Plastic ABS (bulk/injection)Plastic POM/AcetalPlastic Nylon PA6Plastic Nylon PA66Plastic PEEKPlastic PTFEPlastic UHMWPEPlastic PolypropylenePlastic PMMAFDM ASAFDM PolycarbonateFDM PAHT-CFFDM HIPSSLA Resin Tough 2000SLA Resin Elastic 50ASLS PA12 NylonDMLS AlSi10Mg AluminumDMLS Ti-6Al-4V ELI TitaniumDMLS 316L Stainless SteelDMLS 17-4PH Stainless SteelBrickPCB Laminate FR-4SiliconCeramic Alumina 96%Aluminum A380Aluminum 6063-T6Aluminum 1100-OAluminum ADC12Magnesium AZ91DSolder SAC305Plastic PBT GF30Plastic PPS GF40Plastic LCP GF30Plastic HDPEPlastic Polycarbonate
Strength against density