Thermal conductivity against densityHigher and further left: spreads more heat for its weightThermal expansion against thermal conductivityLower and further right: warps less when heated
Try it on a partA bracket to run stress or thermal on, free in your browser
Sources3 documents: Cleveland-Cliffs, Formlabs, National Institute of Standards and Technology
Iron
Cleveland-Cliffs / AK Steel ARMCO Pure Iron Product Data Bulletin (07/2022): Table 1 typical physical properties, Table 2 typical mechanical properties after SRA/recrystallization anneal.
SLA Resin Tough 2000
Formlabs Tough 2000 Resin V2 (FLTO2002), TDS Rev. 01 10/06/2025; printed on Form 4 at 100 µm, washed in Form Wash V2 10+5 min in >=99% IPA, post-cured 70 °C for 12 min in Form Cure V2. Orientation not stated.
1
ARMCO Pure Iron Product Data Bulletin (2022)Cleveland-Cliffsarchived copyIron · Yield strength: typical (0.2% YS), hot rolled + SRA/recrystallization annealIron · Ultimate tensile strength: typical, SRA/recrystallization annealIron · Elongation at break: typical, gauge 4D0Iron · Young's modulus (stiffness): typical, after SRA/recrystallization annealIron · Density: typicalIron · Thermal conductivity: typical at 20 °CIron · Thermal expansion: mean, 20-399 °CIron · Specific heat: typicalIron · Melting point: typical
Elastic Properties of Metals and Alloys, I. Iron, Nickel, and Iron-Nickel Alloys, J. Phys. Chem. Ref. Data 2 (1973)National Institute of Standards and Technologyarchived copyIron · Poisson's ratio: NIST critically evaluated best value (polycrystalline iron)
Each number points to the document that states it, with the exact basis. Values without a number are computed from the sourced ones. "Not sourced" means no citable source states it (or only a specification minimum); figures computed from it are left out too.
SLA Resin Tough 2000 is 3D printed: its properties depend on build direction and print settings; these are typical values.
Questions
Mechanical
Is Iron stronger than SLA Resin Tough 2000?
Iron is stronger: its yield strength is 186 MPa against 40.4 MPa for SLA Resin Tough 2000 (4.6x).
Which is lighter, Iron or SLA Resin Tough 2000?
SLA Resin Tough 2000 is lighter: 1,090 kg/m³ against 7,860 kg/m³ for Iron.
Which is stiffer, Iron or SLA Resin Tough 2000?
Iron is stiffer: Young's modulus 207 GPa against 1.8 GPa for SLA Resin Tough 2000, so the same part in Iron deflects less under the same load.
Which is lighter for the same job, Iron or SLA Resin Tough 2000?
For the same stiffness or strength: Iron is lighter for a stiff rod or tie (tension), stiff beam (bending); SLA Resin Tough 2000 is lighter for a stiff panel or plate, strong rod or tie, strong beam, strong panel or plate.
Part that must be
Iron
SLA Resin Tough 2000
Stiff rod or tie (tension)
lighter
15.9x heavier
Stiff beam (bending)
lighter
49% heavier
Stiff panel or plate
48% heavier
lighter
Strong rod or tie
1.57x heavier
lighter
Strong beam
2.61x heavier
lighter
Strong panel or plate
3.36x heavier
lighter
For the same stiffness or strength, mass scales with density over stiffness (or strength) raised to a power set by how the part is loaded: 1 for a rod in tension, 1/2 for a beam in bending, 1/3 for a panel (the standard material-selection indices).
Which is more ductile, Iron or SLA Resin Tough 2000?
SLA Resin Tough 2000 stretches further before it breaks: 79% elongation at break against 38% for Iron.
Thermal
Which expands less with temperature?
Iron expands less: 13.7 µm/m·K against 134 µm/m·K for SLA Resin Tough 2000.